General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 8.57 g/cm³ Show Material materials with Densidad of 8.57 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Vickers 10 | 20.0 °C | 60 [-] Show Material materials with Dureza Vickers 10 of 60 [-] |
Elongation A25 | 20.0 °C | 30 % Show Material materials with Elongation A25 of 30 % |
Límite elástico Rp 0,2 | 20.0 °C | 50 MPa Show Material materials with Límite elástico Rp 0,2 of 50 MPa |
Módulo elástico | 20.0 °C | 103 GPa Show Material materials with Módulo elástico of 103 GPa |
Resistencia a la tracción | 20.0 °C | 95 MPa Show Material materials with Resistencia a la tracción of 95 MPa |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Conductividad térmica | 20.0 °C | 52 W/(m·K) Show Material materials with Conductividad térmica of 52 W/(m·K) |
1000.0 °C | 65 W/(m·K) Show Material materials with Conductividad térmica of 65 W/(m·K) | |
Eléctrico
Property | Temperature | Value |
---|---|---|
Resistividad eléctrica | 20.0 °C | 1.5E-7 Ω·m Show Material materials with Resistividad eléctrica of 1.5E-7 Ω·m |
Chemical properties
Property | Value |
---|---|
Aluminio | 5E-3 % Show Material materials with Aluminio of 5E-3 % |
Carbono | 0.01 % Show Material materials with Carbono of 0.01 % |
Circonio | 0.8 - 1.2 % Show Material materials with Circonio of 0.8 - 1.2 % |
Hafmio | 0.02 % Show Material materials with Hafmio of 0.02 % |
Hidrógeno | 1.5E-3 % Show Material materials with Hidrógeno of 1.5E-3 % |
Hierro | 0.01 % Show Material materials with Hierro of 0.01 % |
Molibdeno | 0.05 % Show Material materials with Molibdeno of 0.05 % |
Nitrógeno | 0.01 % Show Material materials with Nitrógeno of 0.01 % |
Níquel | 5E-3 % Show Material materials with Níquel of 5E-3 % |
Oxígeno | 0.03 % Show Material materials with Oxígeno of 0.03 % |
Silicona | 5E-3 % Show Material materials with Silicona of 5E-3 % |
Titanio | 0.03 % Show Material materials with Titanio of 0.03 % |
Tántalo | 0.5 % Show Material materials with Tántalo of 0.5 % |
Wolframio | 0.05 % Show Material materials with Wolframio of 0.05 % |