Property | Temperature | Value |
---|---|---|
Elongación A50 | 20.0 °C | 22 % Show Material materials with Elongación A50 of 22 % |
315.0 °C | 32 % Show Material materials with Elongación A50 of 32 % | |
Límite elástico Rp 0,2 | 20.0 °C | 150 MPa Show Material materials with Límite elástico Rp 0,2 of 150 MPa |
315.0 °C | 75 MPa Show Material materials with Límite elástico Rp 0,2 of 75 MPa | |
Resistencia a la tracción | 20.0 °C | 400 MPa Show Material materials with Resistencia a la tracción of 400 MPa |
315.0 °C | 170 MPa Show Material materials with Resistencia a la tracción of 170 MPa | |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.01 % Show Material materials with Aluminio of 0.01 % |
Carbono | 0.015 % Show Material materials with Carbono of 0.015 % |
Cobre | 0.01 % Show Material materials with Cobre of 0.01 % |
Cromo | 0.01 % Show Material materials with Cromo of 0.01 % |
Estaño | 5E-3 % Show Material materials with Estaño of 5E-3 % |
Hidrógeno | 2.5E-3 % Show Material materials with Hidrógeno of 2.5E-3 % |
Hierro | 0.05 % Show Material materials with Hierro of 0.05 % |
Molibdeno | 2E-3 % Show Material materials with Molibdeno of 2E-3 % |
Niobio | 0.01 % Show Material materials with Niobio of 0.01 % |
Nitrógeno | 0.01 % Show Material materials with Nitrógeno of 0.01 % |
Níquel | 5E-3 % Show Material materials with Níquel of 5E-3 % |
Oxígeno | 0.04 % Show Material materials with Oxígeno of 0.04 % |
Silicona | 0.01 % Show Material materials with Silicona of 0.01 % |
Titanio | 0.01 % Show Material materials with Titanio of 0.01 % |
Tántalo | 0.02 % Show Material materials with Tántalo of 0.02 % |
Uranio | 1E-3 % Show Material materials with Uranio of 1E-3 % |
Vanadio | 5E-3 % Show Material materials with Vanadio of 5E-3 % |
Wolframio | 0.02 % Show Material materials with Wolframio of 0.02 % |