General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 6.57 g/cm³ Show Material materials with Densidad of 6.57 g/cm³ | Typical for Zirconium |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.34 [-] Show Material materials with Coeficiente de Poisson of 0.34 [-] | Typical for Zirconium |
Dureza Brinell | 20.0 °C | 235 [-] Show Material materials with Dureza Brinell of 235 [-] | |
Dureza Rockwell B | 20.0 °C | 99 [-] Show Material materials with Dureza Rockwell B of 99 [-] | |
Elongación A50 | 20.0 °C | 12 % Show Material materials with Elongación A50 of 12 % | |
Límite elástico Rp 0,2 | 20.0 °C | 345 MPa Show Material materials with Límite elástico Rp 0,2 of 345 MPa | |
Módulo de cizallamiento | 23.0 °C | 35 GPa Show Material materials with Módulo de cizallamiento of 35 GPa | Typical for Zirconium |
Módulo elástico | 23.0 °C | 68 GPa Show Material materials with Módulo elástico of 68 GPa | Typical for Zirconium |
Resistencia a la tracción | 20.0 °C | 483 MPa Show Material materials with Resistencia a la tracción of 483 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 281 - 289 J/(kg·K) Show Material materials with Calor específico of 281 - 289 J/(kg·K) | Typical for Zirconium |
Coeficiente de dilatación térmica | 23.0 °C | 5.7E-6 - 7E-6 1/K Show Material materials with Coeficiente de dilatación térmica of 5.7E-6 - 7E-6 1/K | Typical for Zirconium |
Conductividad térmica | 23.0 °C | 19 - 27 W/(m·K) Show Material materials with Conductividad térmica of 19 - 27 W/(m·K) | Typical for Zirconium |
Temperatura de fusión | 1845 °C Show Material materials with Temperatura de fusión of 1845 °C | Typical for Zirconium |
Chemical properties
Property | Value |
---|---|
Carbono | 0.1 % Show Material materials with Carbono of 0.1 % |
Fósforo | 0.01 % Show Material materials with Fósforo of 0.01 % |
Hafmio | 4.5 % Show Material materials with Hafmio of 4.5 % |
Hidrógeno | 5E-3 % Show Material materials with Hidrógeno of 5E-3 % |
Niobio | 2 - 3 % Show Material materials with Niobio of 2 - 3 % |
Nitrógeno | 0.03 % Show Material materials with Nitrógeno of 0.03 % |
Oxígeno | 0.3 % Show Material materials with Oxígeno of 0.3 % |