Chemical properties
Property | Value |
---|---|
Aluminio | 0.05 % Show Material materials with Aluminio of 0.05 % |
Carbono | 0.025 % Show Material materials with Carbono of 0.025 % |
Cromo | 0.05 % Show Material materials with Cromo of 0.05 % |
Hidrógeno | 5E-3 % Show Material materials with Hidrógeno of 5E-3 % |
Hierro | 0.08 % Show Material materials with Hierro of 0.08 % |
Nitrógeno | 0.02 % Show Material materials with Nitrógeno of 0.02 % |
Oxígeno | 0.13 % Show Material materials with Oxígeno of 0.13 % |
Silicona | 0.05 % Show Material materials with Silicona of 0.05 % |
Titanio | 0.05 % Show Material materials with Titanio of 0.05 % |
Wolframio | 0.02 % Show Material materials with Wolframio of 0.02 % |