Matmatch uses cookies and similar technologies to improve your experience and measure your interactions with our website. We also use them to provide you more relevant information and improve our platform and search tools. If that’s okay, click “Accept all.” To change your preferences, click “Open cookie settings.” You will find more information about cookies on our privacy policy page.
Open cookie settings
Materiales
Categories
No estás conectado
Categories
Encontrar proveedores de metales
List Your Company
Case Studies
Tools
Sobre nosotros
ASTM B777 Class 1 soft annealed (+A)
Los datos sobre este material han sido proporcionados por WIAM.
See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.
All categories
Let us help you find the best supplier!
Metals With High Melting Points
Molybdenum (Mo)
Nanoindentation: Cutting-edge Hardness Measurement for Advanced Materials
Rhenium: Properties, Production, and Applications
Tantalum: Properties, Processing, and Applications
Tungsten Suppliers and Manufacturers
Tungsten: Properties, Production, and Applications
List your company on Matmatch now and reach engineers around the world looking for such materials.
Request more informationGeneral
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 16.85 - 17.3 g/cm³ Show Material materials with Densidad of 16.85 - 17.3 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Rockwell C | 20.0 °C | 32 [-] Show Material materials with Dureza Rockwell C of 32 [-] |
Módulo de cizallamiento | 20.0 °C | 125 - 140 GPa Show Material materials with Módulo de cizallamiento of 125 - 140 GPa |
Módulo elástico | 20.0 °C | 330 - 340 GPa Show Material materials with Módulo elástico of 330 - 340 GPa |
Chemical properties
Property | Value |
---|---|
Wolframio | 90 % Show Material materials with Wolframio of 90 % |
MATMATCH
We connect engineers, product designers and procurement teams with the best materials and suppliers for their job.