General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 17.75 - 18.35 g/cm³ Show Material materials with Densidad of 17.75 - 18.35 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Rockwell C | 20.0 °C | 34 [-] Show Material materials with Dureza Rockwell C of 34 [-] |
Elongación | 20.0 °C | 1 - 3 % Show Material materials with Elongación of 1 - 3 % |
Límite elástico Rp 0,2 | 20.0 °C | 517 MPa Show Material materials with Límite elástico Rp 0,2 of 517 MPa |
Módulo de cizallamiento | 20.0 °C | 140 - 150 GPa Show Material materials with Módulo de cizallamiento of 140 - 150 GPa |
Módulo elástico | 20.0 °C | 360 - 380 GPa Show Material materials with Módulo elástico of 360 - 380 GPa |
Resistencia a la tracción | 20.0 °C | 648 - 724 MPa Show Material materials with Resistencia a la tracción of 648 - 724 MPa |
Chemical properties
Property | Value |
---|---|
Wolframio | 95 % Show Material materials with Wolframio of 95 % |