General
Property | Value | Comment |
---|---|---|
Densidad | 4.506 g/cm³ Show Material materials with Densidad of 4.506 g/cm³ | Typical for Pure Titanium |
Mecánica
Property | Value | Comment |
---|---|---|
Coeficiente de Poisson | 0.361 [-] Show Material materials with Coeficiente de Poisson of 0.361 [-] | Typical for Pure Titanium |
Módulo de cizallamiento | 46.0 GPa Show Material materials with Módulo de cizallamiento of 46.0 GPa | Typical for Pure Titanium |
Módulo elástico | 120.0 GPa Show Material materials with Módulo elástico of 120.0 GPa | Typical for Pure Titanium |
Aplicaciones térmicas
Property | Temperature | Value | Related Standards | Comment |
---|---|---|---|---|
Calor específico | 513.0 - 599.0 J/(kg·K) Show Material materials with Calor específico of 513.0 - 599.0 J/(kg·K) | Typical for Pure Titanium | ||
Coeficiente de dilatación térmica | 8.400000000000001e-06 - 8.599999999999999e-06 1/K Show Material materials with Coeficiente de dilatación térmica of 8.400000000000001e-06 - 8.599999999999999e-06 1/K | Typical for Pure Titanium | ||
Conductividad térmica | 20.0 °C | 16.3 W/(m·K) Show Material materials with Conductividad térmica of 16.3 W/(m·K) | DIN 17865 | |
Temperatura de fusión | 1670.0 °C Show Material materials with Temperatura de fusión of 1670.0 °C | Typical for Pure Titanium |
Eléctrico
Property | Temperature | Value | Related Standards |
---|---|---|---|
Conductividad eléctrica | 20.0 °C | 1750000.0 S/m Show Material materials with Conductividad eléctrica of 1750000.0 S/m | DIN 17865 |
Chemical properties
Property | Value | Related Standards |
---|---|---|
Carbono | 0.1 Show Material materials with Carbono of 0.1 | DIN 17865 |
Hidrógeno | 0.015 Show Material materials with Hidrógeno of 0.015 | DIN 17865 |
Hierro | 0.2 Show Material materials with Hierro of 0.2 | DIN 17865 |
Nitrógeno | 0.05 Show Material materials with Nitrógeno of 0.05 | DIN 17865 |
Oxígeno | 0.4 Show Material materials with Oxígeno of 0.4 | DIN 17865 |
Paladio | 0.15 - 0.25 % Show Material materials with Paladio of 0.15 - 0.25 % | DIN 17865 |