General
Property | Value | Comment |
---|---|---|
Densidad | 4.506 g/cm³ Show Material materials with Densidad of 4.506 g/cm³ | Typical for Titanium |
Mecánica
Property | Temperature | Value | Condition | Related Standards | Comment |
---|---|---|---|---|---|
Elongación | 20.0 °C | 12.0 % Show Material materials with Elongación of 12.0 % | As-Cast | DIN 17865 | |
Módulo elástico | 100.0 - 120.0 GPa Show Material materials with Módulo elástico of 100.0 - 120.0 GPa | Typical for Titanium Near Alpha Alloy | |||
Resistencia a la tracción | 20.0 °C | 450.0 MPa Show Material materials with Resistencia a la tracción of 450.0 MPa | As-Cast | DIN 17865 |
Aplicaciones térmicas
Property | Temperature | Value | Condition | Related Standards | Comment |
---|---|---|---|---|---|
Calor específico | 460.0 - 527.0 J/(kg·K) Show Material materials with Calor específico of 460.0 - 527.0 J/(kg·K) | Typical for Titanium Near Alpha Alloy | |||
Coeficiente de dilatación térmica | 7.599999999999997e-06 - 1.1e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 7.599999999999997e-06 - 1.1e-05 1/K | Typical for Titanium Near Alpha Alloy | |||
Conductividad térmica | 20.0 °C | 16.3 W/(m·K) Show Material materials with Conductividad térmica of 16.3 W/(m·K) | As-Cast | DIN 17865 | |
Temperatura de fusión | 1540.0 - 1715.0 °C Show Material materials with Temperatura de fusión of 1540.0 - 1715.0 °C | Typical for Titanium Near Alpha Alloy |
Eléctrico
Property | Temperature | Value | Condition | Related Standards |
---|---|---|---|---|
Conductividad eléctrica | 20.0 °C | 1750000.0 S/m Show Material materials with Conductividad eléctrica of 1750000.0 S/m | As-Cast | DIN 17865 |
Chemical properties
Property | Value | Condition | Related Standards |
---|---|---|---|
Carbono | 0.1 Show Material materials with Carbono of 0.1 | As-Cast | DIN 17865 |
Hidrógeno | 0.015 Show Material materials with Hidrógeno of 0.015 | As-Cast | DIN 17865 |
Hierro | 0.25 Show Material materials with Hierro of 0.25 | As-Cast | DIN 17865 |
Nitrógeno | 0.05 Show Material materials with Nitrógeno of 0.05 | As-Cast | DIN 17865 |
Oxígeno | 0.4 Show Material materials with Oxígeno of 0.4 | As-Cast | DIN 17865 |
Technological properties
Property | ||
---|---|---|
Processing methods | investment casting, compact casting, separately cast test samples or taken from casting without ingate |