General
Property | Value | Comment |
---|---|---|
Densidad | 4.506 g/cm³ Show Material materials with Densidad of 4.506 g/cm³ | Typical for Titanium |
Mecánica
Property | Temperature | Value | Condition | Related Standards | Comment |
---|---|---|---|---|---|
Elongación | 20.0 °C | 5.0 % Show Material materials with Elongación of 5.0 % | As-Cast | DIN 17865 | |
Módulo elástico | 120.0 GPa Show Material materials with Módulo elástico of 120.0 GPa | Typical for Titanium | |||
Resistencia a la tracción | 20.0 °C | 880.0 MPa Show Material materials with Resistencia a la tracción of 880.0 MPa | As-Cast | DIN 17865 |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Coeficiente de dilatación térmica | 8.400000000000001e-06 - 8.599999999999999e-06 1/K Show Material materials with Coeficiente de dilatación térmica of 8.400000000000001e-06 - 8.599999999999999e-06 1/K | Typical for Titanium |
Temperatura de fusión | 1668.0 °C Show Material materials with Temperatura de fusión of 1668.0 °C | Typical for Titanium |
Chemical properties
Property | Value | Condition | Related Standards |
---|---|---|---|
Aluminio | 5.5 - 6.5 % Show Material materials with Aluminio of 5.5 - 6.5 % | As-Cast | DIN 17865 |
Carbono | 0.1 Show Material materials with Carbono of 0.1 | As-Cast | DIN 17865 |
Circonio | 3.6 - 4.4 % Show Material materials with Circonio of 3.6 - 4.4 % | As-Cast | DIN 17865 |
Estaño | 1.8 - 2.2 % Show Material materials with Estaño of 1.8 - 2.2 % | As-Cast | DIN 17865 |
Hidrógeno | 0.015 Show Material materials with Hidrógeno of 0.015 | As-Cast | DIN 17865 |
Hierro | 0.25 Show Material materials with Hierro of 0.25 | As-Cast | DIN 17865 |
Molibdeno | 1.8 - 2.2 % Show Material materials with Molibdeno of 1.8 - 2.2 % | As-Cast | DIN 17865 |
Nitrógeno | 0.05 Show Material materials with Nitrógeno of 0.05 | As-Cast | DIN 17865 |
Oxígeno | 0.2 Show Material materials with Oxígeno of 0.2 | As-Cast | DIN 17865 |
Silicona | 0.06 - 0.12 % Show Material materials with Silicona of 0.06 - 0.12 % | As-Cast | DIN 17865 |
Technological properties
Property | ||
---|---|---|
Processing methods | investment casting, compact casting, separately cast test samples or taken from casting without ingate |