General
Property | Value | Comment |
---|---|---|
Densidad | 4.506 g/cm³ Show Material materials with Densidad of 4.506 g/cm³ | Typical for Titanium |
Mecánica
Property | Temperature | Value | Condition | Related Standards | Comment |
---|---|---|---|---|---|
Elongación | 20.0 °C | 5.0 % Show Material materials with Elongación of 5.0 % | Annealed | WL 3.7264-1, DIN 17865 | |
Estricción | 20.0 °C | 10.0 % Show Material materials with Estricción of 10.0 % | Annealed | WL 3.7264-1, DIN 17865 | |
Módulo elástico | 120.0 GPa Show Material materials with Módulo elástico of 120.0 GPa | Typical for Titanium | |||
Resistencia a la tracción | 20.0 °C | 880.0 MPa Show Material materials with Resistencia a la tracción of 880.0 MPa | Annealed | WL 3.7264-1, DIN 17865 |
Aplicaciones térmicas
Property | Temperature | Value | Condition | Related Standards | Comment |
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 8.400000000000001e-06 - 8.599999999999999e-06 1/K Show Material materials with Coeficiente de dilatación térmica of 8.400000000000001e-06 - 8.599999999999999e-06 1/K | Typical for Titanium | |||
Conductividad térmica | 20.0 °C | 7.1 W/(m·K) Show Material materials with Conductividad térmica of 7.1 W/(m·K) | Annealed | WL 3.7264-1, DIN 17865 | |
Temperatura de fusión | 1668.0 °C Show Material materials with Temperatura de fusión of 1668.0 °C | Typical for Titanium |
Eléctrico
Property | Temperature | Value | Condition | Related Standards |
---|---|---|---|---|
Conductividad eléctrica | 20.0 °C | 580000.0 S/m Show Material materials with Conductividad eléctrica of 580000.0 S/m | Annealed | WL 3.7264-1, DIN 17865 |
Chemical properties
Property | Value | Condition | Related Standards |
---|---|---|---|
Aluminio | 5.5 - 6.7 % Show Material materials with Aluminio of 5.5 - 6.7 % | Annealed | WL 3.7264-1, DIN 17865 |
Carbono | 0.1 Show Material materials with Carbono of 0.1 | Annealed | WL 3.7264-1, DIN 17865 |
Hidrógeno | 0.015 Show Material materials with Hidrógeno of 0.015 | Annealed | WL 3.7264-1, DIN 17865 |
Hierro | 0.3 Show Material materials with Hierro of 0.3 | Annealed | WL 3.7264-1, DIN 17865 |
Nitrógeno | 0.05 Show Material materials with Nitrógeno of 0.05 | Annealed | WL 3.7264-1, DIN 17865 |
Oxígeno | 0.25 Show Material materials with Oxígeno of 0.25 | Annealed | WL 3.7264-1, DIN 17865 |
Titanio | 87.7 % Show Material materials with Titanio of 87.7 % | Annealed | WL 3.7264-1, DIN 17865 |
Vanadio | 3.5 - 4.5 % Show Material materials with Vanadio of 3.5 - 4.5 % | Annealed | WL 3.7264-1, DIN 17865 |
Technological properties
Property | ||
---|---|---|
Processing methods | investment casting, sample taken from casting or separately cast or cast on |