Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.13 g/cm³ Show Material materials with Densidad of 7.13 g/cm³ | Typical for Zinc |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.25 [-] Show Material materials with Coeficiente de Poisson of 0.25 [-] | Typical for Zinc |
Dureza Vickers | 20.0 °C | 40 [-] Show Material materials with Dureza Vickers of 40 [-] | |
Elongation A10 | 20.0 °C | 35 - 40 % Show Material materials with Elongation A10 of 35 - 40 % | |
Límite elástico Rp 0,2 | 20.0 °C | 100 MPa Show Material materials with Límite elástico Rp 0,2 of 100 MPa | |
Módulo de cizallamiento | 23.0 °C | 42 GPa Show Material materials with Módulo de cizallamiento of 42 GPa | Typical for Zinc |
Módulo elástico | 23.0 °C | 105 GPa Show Material materials with Módulo elástico of 105 GPa | Typical for Zinc |
Resistencia a la tracción | 20.0 °C | 150 MPa Show Material materials with Resistencia a la tracción of 150 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 272 - 525 J/(kg·K) Show Material materials with Calor específico of 272 - 525 J/(kg·K) | Typical for Zinc |
Coeficiente de dilatación térmica | 23.0 °C | 2.2E-5 - 2.8E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 2.2E-5 - 2.8E-5 1/K | Typical for Zinc |
Conductividad térmica | 23.0 °C | 105 - 125 W/(m·K) Show Material materials with Conductividad térmica of 105 - 125 W/(m·K) | Typical for Zinc |
Temperatura de fusión | 380 - 420 °C Show Material materials with Temperatura de fusión of 380 - 420 °C | Typical for Zinc |
Chemical properties
Property | Value |
---|---|
Cadmio | 3E-3 % Show Material materials with Cadmio of 3E-3 % |
Cobre | 1E-3 % Show Material materials with Cobre of 1E-3 % |
Estaño | 1E-3 % Show Material materials with Estaño of 1E-3 % |
Hierro | 2E-3 % Show Material materials with Hierro of 2E-3 % |
Plomo | 3E-3 % Show Material materials with Plomo of 3E-3 % |
Zinc | 100 % Show Material materials with Zinc of 100 % |