General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 5 g/cm³ Show Material materials with Densidad of 5 g/cm³ | Typical for Zinc Aluminium |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Zinc Aluminium |
Dureza Brinell | 20.0 °C | 40 - 50 [-] Show Material materials with Dureza Brinell of 40 - 50 [-] | |
Elongation A10 | 20.0 °C | 60 - 80 % Show Material materials with Elongation A10 of 60 - 80 % | |
Resistencia a la tracción | 20.0 °C | 200 - 240 MPa Show Material materials with Resistencia a la tracción of 200 - 240 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 393 - 525 J/(kg·K) Show Material materials with Calor específico of 393 - 525 J/(kg·K) | Typical for Zinc Aluminium |
Coeficiente de dilatación térmica | 23.0 °C | 2.2E-5 - 2.8E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 2.2E-5 - 2.8E-5 1/K | Typical for Zinc Aluminium |
Conductividad térmica | 23.0 °C | 105 - 125 W/(m·K) Show Material materials with Conductividad térmica of 105 - 125 W/(m·K) | Typical for Zinc Aluminium |
Temperatura de fusión | 375 - 485 °C Show Material materials with Temperatura de fusión of 375 - 485 °C | Typical for Zinc Aluminium |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.7 - 0.9 % Show Material materials with Aluminio of 0.7 - 0.9 % |
Cobre | 0.3 - 0.5 % Show Material materials with Cobre of 0.3 - 0.5 % |
Zinc | 98.6 % Show Material materials with Zinc of 98.6 % |