General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 5 g/cm³ Show Material materials with Densidad of 5 g/cm³ | Typical for Zinc Aluminium |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Zinc Aluminium |
Dureza Brinell | 20.0 °C | 90 - 110 [-] Show Material materials with Dureza Brinell of 90 - 110 [-] | |
Elongation A10 | 20.0 °C | 8 - 12 % Show Material materials with Elongation A10 of 8 - 12 % | |
Resistencia a la tracción | 20.0 °C | 400 - 460 MPa Show Material materials with Resistencia a la tracción of 400 - 460 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 393 - 525 J/(kg·K) Show Material materials with Calor específico of 393 - 525 J/(kg·K) | Typical for Zinc Aluminium |
Coeficiente de dilatación térmica | 23.0 °C | 2.2E-5 - 2.8E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 2.2E-5 - 2.8E-5 1/K | Typical for Zinc Aluminium |
Conductividad térmica | 23.0 °C | 105 - 125 W/(m·K) Show Material materials with Conductividad térmica of 105 - 125 W/(m·K) | Typical for Zinc Aluminium |
Temperatura de fusión | 375 - 485 °C Show Material materials with Temperatura de fusión of 375 - 485 °C | Typical for Zinc Aluminium |
Chemical properties
Property | Value |
---|---|
Aluminio | 9 - 11 % Show Material materials with Aluminio of 9 - 11 % |
Cobre | 0.6 - 1 % Show Material materials with Cobre of 0.6 - 1 % |
Magnesio | 0.02 - 0.05 % Show Material materials with Magnesio of 0.02 - 0.05 % |
Zinc | 87.95 % Show Material materials with Zinc of 87.95 % |