General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 11.34 g/cm³ Show Material materials with Densidad of 11.34 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.4 [-] Show Material materials with Coeficiente de Poisson of 0.4 [-] | Typical for Pure/Low Alloyed Lead |
Módulo elástico | 20.0 °C | 17 GPa Show Material materials with Módulo elástico of 17 GPa | |
Resistencia a la tracción | 20.0 °C | 14 MPa Show Material materials with Resistencia a la tracción of 14 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 112 - 134 J/(kg·K) Show Material materials with Calor específico of 112 - 134 J/(kg·K) | Typical for Pure/Low Alloyed Lead |
Conductividad térmica | 23.0 °C | 34 - 35 W/(m·K) Show Material materials with Conductividad térmica of 34 - 35 W/(m·K) | Typical for Pure/Low Alloyed Lead |
Temperatura de fusión | 327 °C Show Material materials with Temperatura de fusión of 327 °C | Typical for Pure/Low Alloyed Lead |
Chemical properties
Property | Value |
---|---|
Antimonio | 1E-3 % Show Material materials with Antimonio of 1E-3 % |
Arsénico | 1E-3 % Show Material materials with Arsénico of 1E-3 % |
Bismuto | 0.01 % Show Material materials with Bismuto of 0.01 % |
Cobre | 0.04 - 0.05 % Show Material materials with Cobre of 0.04 - 0.05 % |
Estaño | 5E-3 % Show Material materials with Estaño of 5E-3 % |
Hierro | 1E-3 % Show Material materials with Hierro of 1E-3 % |
Plata | 5E-3 % Show Material materials with Plata of 5E-3 % |
Plomo | 99.99 % Show Material materials with Plomo of 99.99 % |
Zinc | 1E-3 % Show Material materials with Zinc of 1E-3 % |