General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 9.6 g/cm³ Show Material materials with Densidad of 9.6 g/cm³ | Typical for Lead Antimony |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 130 - 159 J/(kg·K) Show Material materials with Calor específico of 130 - 159 J/(kg·K) | Typical for Lead Antimony |
Conductividad térmica | 23.0 °C | 24 - 34 W/(m·K) Show Material materials with Conductividad térmica of 24 - 34 W/(m·K) | Typical for Lead Antimony |
Temperatura de fusión | 235 - 305 °C Show Material materials with Temperatura de fusión of 235 - 305 °C | Typical for Lead Antimony |
Chemical properties
Property | Value |
---|---|
Antimonio | 0.15 - 0.25 % Show Material materials with Antimonio of 0.15 - 0.25 % |
Arsénico | 1E-3 % Show Material materials with Arsénico of 1E-3 % |
Bismuto | 0.03 % Show Material materials with Bismuto of 0.03 % |
Cadmio | 1E-3 % Show Material materials with Cadmio of 1E-3 % |
Cobre | 3E-3 % Show Material materials with Cobre of 3E-3 % |
Estaño | 0.35 - 0.45 % Show Material materials with Estaño of 0.35 - 0.45 % |
Níquel | 1E-3 % Show Material materials with Níquel of 1E-3 % |
Plata | 5E-3 % Show Material materials with Plata of 5E-3 % |
Plomo | 99.26 % Show Material materials with Plomo of 99.26 % |
Telurio | 2E-3 % Show Material materials with Telurio of 2E-3 % |
Zinc | 1E-3 % Show Material materials with Zinc of 1E-3 % |