General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 6.5 g/cm³ Show Material materials with Densidad of 6.5 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Zinc Aluminium |
Dureza Brinell | 20.0 °C | 80 - 90 [-] Show Material materials with Dureza Brinell of 80 - 90 [-] | |
Elongación | 20.0 °C | 1 - 3 % Show Material materials with Elongación of 1 - 3 % | |
Límite elástico Rp 0,2 | 20.0 °C | 150 - 200 MPa Show Material materials with Límite elástico Rp 0,2 of 150 - 200 MPa | |
Módulo elástico | 20.0 °C | 130 GPa Show Material materials with Módulo elástico of 130 GPa | |
Resistencia a la tracción | 20.0 °C | 180 - 260 MPa Show Material materials with Resistencia a la tracción of 180 - 260 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 20.0 °C | 452 J/(kg·K) Show Material materials with Calor específico of 452 J/(kg·K) | |
Coeficiente de dilatación térmica | 23.0 °C | 2.2E-5 - 2.8E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 2.2E-5 - 2.8E-5 1/K | Typical for Zinc Aluminium |
Conductividad térmica | 20.0 °C | 105 W/(m·K) Show Material materials with Conductividad térmica of 105 W/(m·K) | |
Temperatura de fusión | 375 - 485 °C Show Material materials with Temperatura de fusión of 375 - 485 °C | Typical for Zinc Aluminium |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 20.0 °C | 1.50E+7 - 1.60E+7 S/m Show Material materials with Conductividad eléctrica of 1.50E+7 - 1.60E+7 S/m |
Chemical properties
Property | Value |
---|---|
Aluminio | 5.6 - 6 % Show Material materials with Aluminio of 5.6 - 6 % |
Cobre | 1.2 - 1.6 % Show Material materials with Cobre of 1.2 - 1.6 % |
Estaño | 2E-3 % Show Material materials with Estaño of 2E-3 % |
Hierro | 0.08 % Show Material materials with Hierro of 0.08 % |
Magnesio | 5E-3 % Show Material materials with Magnesio of 5E-3 % |
Zinc | 92.32 % Show Material materials with Zinc of 92.32 % |
Technological properties
Property | ||
---|---|---|
Processing methods | permanent mould casting, separately cast test sample |