Zinkberatung e. V. 1981 Grade G-ZnAl27Cu2 heat treated

Want to keep this datasheet? Save it now in your required format

Description

The material ZnAl27Cu2, a fine zinc block metal alloy acc. to ASTM B 669, german marking ZA 27, is used with the transition coming from malleable cast iron or cast iron with nodular graphite, brass or bronze, where it depends on highest strength and strain. ZA 27 is the best alloy for operatings temperature to 120 °C. The alloy is pressure tight, even in thin cross sections. Where however highest pressure tight ones is necessary, the alloys ZnAl8 or ZnAl12 should be considered. The material is excellently machinable and on high polish sharpening and polishingable. The alloy is used mainly for sand and ingot casting, in addition, for pressure casting on cold chamber machines.

Equivalent Materials

Los datos sobre este material han sido proporcionados por WIAM.

A menos que se indique lo contrario, todas las medidas corresponden a condiciones de temperatura ambiente. A menos que se indique lo contrario, se utilizan las unidades del SI.
Las normas armonizadas son similares a uno o varios estándares del proveedor. Es posible que algunas normas armonizadas se ajusten al estándar original, mientras que otras pueden quedar fuera de su alcance.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Propiedades

General

PropertyTemperatureValue

Densidad

20.0 °C

5 g/cm³

Show Material materials with Densidad of 5 g/cm³

Mecánica

PropertyTemperatureValueComment

Coeficiente de Poisson

23.0 °C

0.3 [-]

Show Material materials with Coeficiente de Poisson of 0.3 [-]

Typical for Zinc Aluminium

Dureza Brinell

20.0 °C

90 - 100 [-]

Show Material materials with Dureza Brinell of 90 - 100 [-]

Elongación A50

20.0 °C

8 - 11 %

Show Material materials with Elongación A50 of 8 - 11 %

Límite elástico Rp 0,2

20.0 °C

254 MPa

Show Material materials with Límite elástico Rp 0,2 of 254 MPa

Módulo elástico

20.0 °C

75 GPa

Show Material materials with Módulo elástico of 75 GPa

Resistencia a la tracción

20.0 °C

310 - 325 MPa

Show Material materials with Resistencia a la tracción of 310 - 325 MPa

Aplicaciones térmicas

PropertyTemperatureValueComment

Calor específico

23.0 °C

393 - 525 J/(kg·K)

Show Material materials with Calor específico of 393 - 525 J/(kg·K)

Typical for Zinc Aluminium

Coeficiente de dilatación térmica

23.0 °C

2.2E-5 - 2.8E-5 1/K

Show Material materials with Coeficiente de dilatación térmica of 2.2E-5 - 2.8E-5 1/K

Typical for Zinc Aluminium

Conductividad térmica

23.0 °C

105 - 125 W/(m·K)

Show Material materials with Conductividad térmica of 105 - 125 W/(m·K)

Typical for Zinc Aluminium

Temperatura de fusión

375 - 485 °C

Show Material materials with Temperatura de fusión of 375 - 485 °C

Typical for Zinc Aluminium

Chemical properties

PropertyValue

Aluminio

25 - 28 %

Show Material materials with Aluminio of 25 - 28 %

Cadmio

3E-3 %

Show Material materials with Cadmio of 3E-3 %

Cobre

2 - 2.5 %

Show Material materials with Cobre of 2 - 2.5 %

Estaño

2E-3 %

Show Material materials with Estaño of 2E-3 %

Hierro

0.1 %

Show Material materials with Hierro of 0.1 %

Magnesio

0.01 - 0.02 %

Show Material materials with Magnesio of 0.01 - 0.02 %

Plomo

4E-3 %

Show Material materials with Plomo of 4E-3 %

Zinc

69.37 %

Show Material materials with Zinc of 69.37 %

Technological properties

Property
Processing methods

sand casting