General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 10.1 g/cm³ Show Material materials with Densidad of 10.1 g/cm³ |
Mecánica
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 130 - 159 J/(kg·K) Show Material materials with Calor específico of 130 - 159 J/(kg·K) | Typical for Lead Antimony |
Conductividad térmica | 23.0 °C | 24 - 34 W/(m·K) Show Material materials with Conductividad térmica of 24 - 34 W/(m·K) | Typical for Lead Antimony |
Temperatura de fusión | 235 - 305 °C Show Material materials with Temperatura de fusión of 235 - 305 °C | Typical for Lead Antimony |
Chemical properties
Property | Value |
---|---|
Antimonio | 12 - 14 % Show Material materials with Antimonio of 12 - 14 % |
Arsénico | 0.05 % Show Material materials with Arsénico of 0.05 % |
Cadmio | 0.05 % Show Material materials with Cadmio of 0.05 % |
Hierro | 0.05 % Show Material materials with Hierro of 0.05 % |
Plomo | 86 - 88 % Show Material materials with Plomo of 86 - 88 % |
Technological properties
Property | ||
---|---|---|
Processing methods | pressure die casting, separately cast test sample,pressure die casting |