General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 10.14 g/cm³ Show Material materials with Densidad of 10.14 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.37 [-] Show Material materials with Coeficiente de Poisson of 0.37 [-] | Typical for Silver |
Dureza Vickers 5 | 20.0 °C | 90 [-] Show Material materials with Dureza Vickers 5 of 90 [-] | |
Elongación | 20.0 °C | 55 % Show Material materials with Elongación of 55 % | |
Módulo de cizallamiento | 23.0 °C | 30 GPa Show Material materials with Módulo de cizallamiento of 30 GPa | Typical for Silver |
Módulo elástico | 23.0 °C | 83 GPa Show Material materials with Módulo elástico of 83 GPa | Typical for Silver |
Resistencia a la tracción | 20.0 °C | 370 MPa Show Material materials with Resistencia a la tracción of 370 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 234 - 251 J/(kg·K) Show Material materials with Calor específico of 234 - 251 J/(kg·K) | Typical for Silver |
Coeficiente de dilatación térmica | 23.0 °C | 1.9E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.9E-5 1/K | Typical for Silver |
Conductividad térmica | 23.0 °C | 417 - 428 W/(m·K) Show Material materials with Conductividad térmica of 417 - 428 W/(m·K) | Typical for Silver |
Temperatura de fusión | 962 °C Show Material materials with Temperatura de fusión of 962 °C | Typical for Silver |