General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 11.2 g/cm³ Show Material materials with Densidad of 11.2 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.37 [-] Show Material materials with Coeficiente de Poisson of 0.37 [-] | Typical for Silver |
Dureza Vickers | 20.0 °C | 160 [-] Show Material materials with Dureza Vickers of 160 [-] | |
Módulo de cizallamiento | 23.0 °C | 30 GPa Show Material materials with Módulo de cizallamiento of 30 GPa | Typical for Silver |
Módulo elástico | 20.0 °C | 137 GPa Show Material materials with Módulo elástico of 137 GPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 234 - 251 J/(kg·K) Show Material materials with Calor específico of 234 - 251 J/(kg·K) | Typical for Silver |
Coeficiente de dilatación térmica | 23.0 °C | 1.9E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.9E-5 1/K | Typical for Silver |
Conductividad térmica | 20.0 °C | 33.5 W/(m·K) Show Material materials with Conductividad térmica of 33.5 W/(m·K) | |
Temperatura de fusión | 962 °C Show Material materials with Temperatura de fusión of 962 °C | Typical for Silver |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 20.0 °C | 3.00E+6 S/m Show Material materials with Conductividad eléctrica of 3.00E+6 S/m |
Resistividad eléctrica | 20.0 °C | 3.33E-7 Ω·m Show Material materials with Resistividad eléctrica of 3.33E-7 Ω·m |