General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 16 g/cm³ Show Material materials with Densidad of 16 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.37 [-] Show Material materials with Coeficiente de Poisson of 0.37 [-] | Typical for Silver |
Dureza Vickers | 20.0 °C | 180 [-] Show Material materials with Dureza Vickers of 180 [-] | |
Módulo de cizallamiento | 23.0 °C | 30 GPa Show Material materials with Módulo de cizallamiento of 30 GPa | Typical for Silver |
Módulo elástico | 23.0 °C | 83 GPa Show Material materials with Módulo elástico of 83 GPa | Typical for Silver |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 234 - 251 J/(kg·K) Show Material materials with Calor específico of 234 - 251 J/(kg·K) | Typical for Silver |
Coeficiente de dilatación térmica | 23.0 °C | 1.9E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.9E-5 1/K | Typical for Silver |
Conductividad térmica | 20.0 °C | 239 W/(m·K) Show Material materials with Conductividad térmica of 239 W/(m·K) | |
Temperatura de fusión | 962 °C Show Material materials with Temperatura de fusión of 962 °C | Typical for Silver |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 20.0 °C | 2.20E+7 S/m Show Material materials with Conductividad eléctrica of 2.20E+7 S/m |
Resistividad eléctrica | 20.0 °C | 4.6E-8 Ω·m Show Material materials with Resistividad eléctrica of 4.6E-8 Ω·m |