General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 16.5 g/cm³ Show Material materials with Densidad of 16.5 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.42 [-] Show Material materials with Coeficiente de Poisson of 0.42 [-] | Typical for Gold |
Dureza Vickers 10 | 20.0 °C | 40 [-] Show Material materials with Dureza Vickers 10 of 40 [-] | |
Módulo de cizallamiento | 20.0 °C | 31 GPa Show Material materials with Módulo de cizallamiento of 31 GPa | |
Módulo elástico | 20.0 °C | 87 GPa Show Material materials with Módulo elástico of 87 GPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 126 - 138 J/(kg·K) Show Material materials with Calor específico of 126 - 138 J/(kg·K) | Typical for Gold |
Coeficiente de dilatación térmica | 300.0 °C | 1.62E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.62E-5 1/K | |
Conductividad térmica | 20.0 °C | 75 W/(m·K) Show Material materials with Conductividad térmica of 75 W/(m·K) | |
Temperatura de fusión | 1064 °C Show Material materials with Temperatura de fusión of 1064 °C | Typical for Gold |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 20.0 °C | 1.00E+7 S/m Show Material materials with Conductividad eléctrica of 1.00E+7 S/m |
Resistividad eléctrica | 20.0 °C | 9.5E-8 - 1E-7 Ω·m Show Material materials with Resistividad eléctrica of 9.5E-8 - 1E-7 Ω·m |