General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 15.4 g/cm³ Show Material materials with Densidad of 15.4 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.42 [-] Show Material materials with Coeficiente de Poisson of 0.42 [-] | Typical for Gold |
Dureza Vickers 10 | 20.0 °C | 83 [-] Show Material materials with Dureza Vickers 10 of 83 [-] | |
Módulo de cizallamiento | 20.0 °C | 37 GPa Show Material materials with Módulo de cizallamiento of 37 GPa | |
Módulo elástico | 20.0 °C | 114 GPa Show Material materials with Módulo elástico of 114 GPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 126 - 138 J/(kg·K) Show Material materials with Calor específico of 126 - 138 J/(kg·K) | Typical for Gold |
Coeficiente de dilatación térmica | 300.0 °C | 1.64E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.64E-5 1/K | |
Conductividad térmica | 20.0 °C | 59 W/(m·K) Show Material materials with Conductividad térmica of 59 W/(m·K) | |
Temperatura de fusión | 1064 °C Show Material materials with Temperatura de fusión of 1064 °C | Typical for Gold |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 20.0 °C | 7.70E+6 - 9.10E+6 S/m Show Material materials with Conductividad eléctrica of 7.70E+6 - 9.10E+6 S/m |
Resistividad eléctrica | 20.0 °C | 1.1E-7 - 1.2E-7 Ω·m Show Material materials with Resistividad eléctrica of 1.1E-7 - 1.2E-7 Ω·m |