General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 18.2 g/cm³ Show Material materials with Densidad of 18.2 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.42 [-] Show Material materials with Coeficiente de Poisson of 0.42 [-] | Typical for Gold |
Dureza Vickers | 20.0 °C | 160 [-] Show Material materials with Dureza Vickers of 160 [-] | |
Módulo de cizallamiento | 23.0 °C | 26 GPa Show Material materials with Módulo de cizallamiento of 26 GPa | Typical for Gold |
Módulo elástico | 20.0 °C | 82 GPa Show Material materials with Módulo elástico of 82 GPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 126 - 138 J/(kg·K) Show Material materials with Calor específico of 126 - 138 J/(kg·K) | Typical for Gold |
Coeficiente de dilatación térmica | 300.0 °C | 1.56E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.56E-5 1/K | |
Conductividad térmica | 20.0 °C | 52 W/(m·K) Show Material materials with Conductividad térmica of 52 W/(m·K) | |
Temperatura de fusión | 1064 °C Show Material materials with Temperatura de fusión of 1064 °C | Typical for Gold |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 20.0 °C | 7.40E+6 S/m Show Material materials with Conductividad eléctrica of 7.40E+6 S/m |
Resistividad eléctrica | 20.0 °C | 1.36E-7 Ω·m Show Material materials with Resistividad eléctrica of 1.36E-7 Ω·m |