Aplicaciones térmicas
Property | Value |
---|---|
Temperatura de fusión | 1040 °C Show Material materials with Temperatura de fusión of 1040 °C |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Vickers 5 | 20.0 °C | 95 [-] Show Material materials with Dureza Vickers 5 of 95 [-] |
Chemical properties
Property | Value |
---|---|
Cobre | 4.1 % Show Material materials with Cobre of 4.1 % |
Oro | 75.7 % Show Material materials with Oro of 75.7 % |
Paladio | 3.3 % Show Material materials with Paladio of 3.3 % |
Plata | 15 % Show Material materials with Plata of 15 % |
Platino | 2 % Show Material materials with Platino of 2 % |
Zinc | 2 % Show Material materials with Zinc of 2 % |