General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 22.4 g/cm³ Show Material materials with Densidad of 22.4 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Coeficiente de Poisson | 20.0 °C | 0.26 [-] Show Material materials with Coeficiente de Poisson of 0.26 [-] |
Dureza Vickers | 20.0 °C | 200 - 300 [-] Show Material materials with Dureza Vickers of 200 - 300 [-] |
Elongación | 20.0 °C | 7 % Show Material materials with Elongación of 7 % |
Límite elástico | 20.0 °C | 93 MPa Show Material materials with Límite elástico of 93 MPa |
Módulo de cizallamiento | 20.0 °C | 210 - 214 GPa Show Material materials with Módulo de cizallamiento of 210 - 214 GPa |
Módulo elástico | -180.0 °C | 560 GPa Show Material materials with Módulo elástico of 560 GPa |
20.0 °C | 528 - 538 GPa Show Material materials with Módulo elástico of 528 - 538 GPa | |
200.0 °C | 520 GPa Show Material materials with Módulo elástico of 520 GPa | |
400.0 °C | 499 GPa Show Material materials with Módulo elástico of 499 GPa | |
500.0 °C | 488 GPa Show Material materials with Módulo elástico of 488 GPa | |
600.0 °C | 478 GPa Show Material materials with Módulo elástico of 478 GPa | |
800.0 °C | 456 GPa Show Material materials with Módulo elástico of 456 GPa | |
900.0 °C | 445 GPa Show Material materials with Módulo elástico of 445 GPa | |
1000.0 °C | 434 GPa Show Material materials with Módulo elástico of 434 GPa | |
Resistencia a la tracción | 20.0 °C | 450 - 1100 MPa Show Material materials with Resistencia a la tracción of 450 - 1100 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 130 - 132 J/(kg·K) Show Material materials with Calor específico of 130 - 132 J/(kg·K) | Typical for Iridium |
Coeficiente de dilatación térmica | 100.0 °C | 6.7E-6 1/K Show Material materials with Coeficiente de dilatación térmica of 6.7E-6 1/K | |
300.0 °C | 7.1E-6 1/K Show Material materials with Coeficiente de dilatación térmica of 7.1E-6 1/K | ||
900.0 °C | 7.8E-6 1/K Show Material materials with Coeficiente de dilatación térmica of 7.8E-6 1/K | ||
1000.0 °C | 7.9E-6 1/K Show Material materials with Coeficiente de dilatación térmica of 7.9E-6 1/K | ||
1100.0 °C | 8E-6 1/K Show Material materials with Coeficiente de dilatación térmica of 8E-6 1/K | ||
1200.0 °C | 8.1E-6 1/K Show Material materials with Coeficiente de dilatación térmica of 8.1E-6 1/K | ||
1300.0 °C | 8.2E-6 1/K Show Material materials with Coeficiente de dilatación térmica of 8.2E-6 1/K | ||
1400.0 °C | 8.4E-6 1/K Show Material materials with Coeficiente de dilatación térmica of 8.4E-6 1/K | ||
1500.0 °C | 8.5E-6 1/K Show Material materials with Coeficiente de dilatación térmica of 8.5E-6 1/K | ||
1600.0 °C | 9.2E-6 1/K Show Material materials with Coeficiente de dilatación térmica of 9.2E-6 1/K | ||
Conductividad térmica | -73.0 °C | 149 W/(m·K) Show Material materials with Conductividad térmica of 149 W/(m·K) | |
20.0 °C | 59 W/(m·K) Show Material materials with Conductividad térmica of 59 W/(m·K) | ||
127.0 °C | 136 W/(m·K) Show Material materials with Conductividad térmica of 136 W/(m·K) | ||
327.0 °C | 130 W/(m·K) Show Material materials with Conductividad térmica of 130 W/(m·K) | ||
527.0 °C | 125 W/(m·K) Show Material materials with Conductividad térmica of 125 W/(m·K) | ||
727.0 °C | 121 W/(m·K) Show Material materials with Conductividad térmica of 121 W/(m·K) | ||
927.0 °C | 117 W/(m·K) Show Material materials with Conductividad térmica of 117 W/(m·K) | ||
1127.0 °C | 110 W/(m·K) Show Material materials with Conductividad térmica of 110 W/(m·K) | ||
1327.0 °C | 106 W/(m·K) Show Material materials with Conductividad térmica of 106 W/(m·K) | ||
1527.0 °C | 103 W/(m·K) Show Material materials with Conductividad térmica of 103 W/(m·K) | ||
Temperatura de fusión | 2447 °C Show Material materials with Temperatura de fusión of 2447 °C | Typical for Iridium |
Eléctrico
Property | Temperature | Value |
---|---|---|
Resistividad eléctrica | 20.0 °C | 4.9E-8 Ω·m Show Material materials with Resistividad eléctrica of 4.9E-8 Ω·m |
Chemical properties
Property | Value |
---|---|
Iridio | 99.9 % Show Material materials with Iridio of 99.9 % |