General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 19.3 g/cm³ Show Material materials with Densidad of 19.3 g/cm³ | Typical for Gold |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.42 [-] Show Material materials with Coeficiente de Poisson of 0.42 [-] | Typical for Gold |
Dureza Vickers 5 | 20.0 °C | 170 [-] Show Material materials with Dureza Vickers 5 of 170 [-] | |
Límite elástico Rp 0,2 | 20.0 °C | 400 MPa Show Material materials with Límite elástico Rp 0,2 of 400 MPa | |
Módulo de cizallamiento | 23.0 °C | 26 GPa Show Material materials with Módulo de cizallamiento of 26 GPa | Typical for Gold |
Módulo elástico | 23.0 °C | 74 - 81 GPa Show Material materials with Módulo elástico of 74 - 81 GPa | Typical for Gold |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 126 - 138 J/(kg·K) Show Material materials with Calor específico of 126 - 138 J/(kg·K) | Typical for Gold |
Coeficiente de dilatación térmica | 23.0 °C | 1.4E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.4E-5 1/K | Typical for Gold |
Conductividad térmica | 23.0 °C | 292 - 316 W/(m·K) Show Material materials with Conductividad térmica of 292 - 316 W/(m·K) | Typical for Gold |
Temperatura de fusión | 1064 °C Show Material materials with Temperatura de fusión of 1064 °C | Typical for Gold |
Chemical properties
Property | Value |
---|---|
Cobre | 12 % Show Material materials with Cobre of 12 % |
Oro | 58 % Show Material materials with Oro of 58 % |
Paladio | 5.5 % Show Material materials with Paladio of 5.5 % |
Plata | 23.3 % Show Material materials with Plata of 23.3 % |
Platino | 2 % Show Material materials with Platino of 2 % |
Zinc | 2 % Show Material materials with Zinc of 2 % |