General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 10.9 g/cm³ Show Material materials with Densidad of 10.9 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.39 [-] Show Material materials with Coeficiente de Poisson of 0.39 [-] | Typical for Palladium |
Dureza Vickers | 20.0 °C | 180 [-] Show Material materials with Dureza Vickers of 180 [-] | |
Elongación | 20.0 °C | 2 % Show Material materials with Elongación of 2 % | |
Límite elástico Rp 0,2 | 20.0 °C | 620 MPa Show Material materials with Límite elástico Rp 0,2 of 620 MPa | |
Módulo de cizallamiento | 20.0 °C | 36 GPa Show Material materials with Módulo de cizallamiento of 36 GPa | |
Módulo elástico | 20.0 °C | 114 GPa Show Material materials with Módulo elástico of 114 GPa | |
Resistencia a la tracción | 20.0 °C | 630 MPa Show Material materials with Resistencia a la tracción of 630 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 236 - 248 J/(kg·K) Show Material materials with Calor específico of 236 - 248 J/(kg·K) | Typical for Palladium |
Coeficiente de dilatación térmica | 300.0 °C | 1.6E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.6E-5 1/K | |
Conductividad térmica | 20.0 °C | 61 W/(m·K) Show Material materials with Conductividad térmica of 61 W/(m·K) | |
Temperatura de fusión | 1553 °C Show Material materials with Temperatura de fusión of 1553 °C | Typical for Palladium |
Eléctrico
Property | Temperature | Value |
---|---|---|
Resistividad eléctrica | 20.0 °C | 1.54E-7 Ω·m Show Material materials with Resistividad eléctrica of 1.54E-7 Ω·m |