General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 10.5 g/cm³ Show Material materials with Densidad of 10.5 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.39 [-] Show Material materials with Coeficiente de Poisson of 0.39 [-] | Typical for Palladium |
Dureza Vickers | 20.0 °C | 220 [-] Show Material materials with Dureza Vickers of 220 [-] | |
Módulo de cizallamiento | 23.0 °C | 42 GPa Show Material materials with Módulo de cizallamiento of 42 GPa | Typical for Palladium |
Módulo elástico | 20.0 °C | 149 GPa Show Material materials with Módulo elástico of 149 GPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 236 - 248 J/(kg·K) Show Material materials with Calor específico of 236 - 248 J/(kg·K) | Typical for Palladium |
Coeficiente de dilatación térmica | 300.0 °C | 1.36E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.36E-5 1/K | |
Conductividad térmica | 20.0 °C | 38 W/(m·K) Show Material materials with Conductividad térmica of 38 W/(m·K) | |
Temperatura de fusión | 1553 °C Show Material materials with Temperatura de fusión of 1553 °C | Typical for Palladium |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 20.0 °C | 3.00E+6 S/m Show Material materials with Conductividad eléctrica of 3.00E+6 S/m |
Resistividad eléctrica | 20.0 °C | 3.33E-7 Ω·m Show Material materials with Resistividad eléctrica of 3.33E-7 Ω·m |