General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 21.5 g/cm³ Show Material materials with Densidad of 21.5 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.39 [-] Show Material materials with Coeficiente de Poisson of 0.39 [-] | Typical for Platinum |
Dureza Vickers | 20.0 °C | 154 [-] Show Material materials with Dureza Vickers of 154 [-] | |
Elongación | 20.0 °C | 2 % Show Material materials with Elongación of 2 % | |
Límite elástico Rp 0,2 | 20.0 °C | 450 MPa Show Material materials with Límite elástico Rp 0,2 of 450 MPa | |
Módulo de cizallamiento | 23.0 °C | 62 GPa Show Material materials with Módulo de cizallamiento of 62 GPa | Typical for Platinum |
Módulo elástico | 20.0 °C | 190 GPa Show Material materials with Módulo elástico of 190 GPa | |
Resistencia a la tracción | 20.0 °C | 470 MPa Show Material materials with Resistencia a la tracción of 470 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 136 J/(kg·K) Show Material materials with Calor específico of 136 J/(kg·K) | Typical for Platinum |
Coeficiente de dilatación térmica | 23.0 °C | 8.8E-6 - 9.1E-6 1/K Show Material materials with Coeficiente de dilatación térmica of 8.8E-6 - 9.1E-6 1/K | Typical for Platinum |
Conductividad térmica | 20.0 °C | 42 W/(m·K) Show Material materials with Conductividad térmica of 42 W/(m·K) | |
Temperatura de fusión | 1769 °C Show Material materials with Temperatura de fusión of 1769 °C | Typical for Platinum |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 20.0 °C | 5.60E+6 S/m Show Material materials with Conductividad eléctrica of 5.60E+6 S/m |
Resistividad eléctrica | 20.0 °C | 1.79E-7 Ω·m Show Material materials with Resistividad eléctrica of 1.79E-7 Ω·m |