General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 20.4 g/cm³ Show Material materials with Densidad of 20.4 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.39 [-] Show Material materials with Coeficiente de Poisson of 0.39 [-] | Typical for Platinum |
Dureza Vickers 10 | 20.0 °C | 115 [-] Show Material materials with Dureza Vickers 10 of 115 [-] | |
Módulo de cizallamiento | 23.0 °C | 62 GPa Show Material materials with Módulo de cizallamiento of 62 GPa | Typical for Platinum |
Módulo elástico | 23.0 °C | 154 - 172 GPa Show Material materials with Módulo elástico of 154 - 172 GPa | Typical for Platinum |
Resistencia a la tracción | 20.0 °C | 360 MPa Show Material materials with Resistencia a la tracción of 360 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 136 J/(kg·K) Show Material materials with Calor específico of 136 J/(kg·K) | Typical for Platinum |
Coeficiente de dilatación térmica | 23.0 °C | 8.8E-6 - 9.1E-6 1/K Show Material materials with Coeficiente de dilatación térmica of 8.8E-6 - 9.1E-6 1/K | Typical for Platinum |
Conductividad térmica | 23.0 °C | 69 - 73 W/(m·K) Show Material materials with Conductividad térmica of 69 - 73 W/(m·K) | Typical for Platinum |
Temperatura de fusión | 1769 °C Show Material materials with Temperatura de fusión of 1769 °C | Typical for Platinum |