General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 12.4 g/cm³ Show Material materials with Densidad of 12.4 g/cm³ | Typical for Rhodium |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.26 [-] Show Material materials with Coeficiente de Poisson of 0.26 [-] | Typical for Rhodium |
Dureza Vickers | 20.0 °C | 235 [-] Show Material materials with Dureza Vickers of 235 [-] | |
Módulo elástico | 23.0 °C | 275 - 290 GPa Show Material materials with Módulo elástico of 275 - 290 GPa | Typical for Rhodium |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 254 J/(kg·K) Show Material materials with Calor específico of 254 J/(kg·K) | Typical for Rhodium |
Coeficiente de dilatación térmica | 23.0 °C | 8.3E-6 - 8.5E-6 1/K Show Material materials with Coeficiente de dilatación térmica of 8.3E-6 - 8.5E-6 1/K | Typical for Rhodium |
Conductividad térmica | 23.0 °C | 88 - 151 W/(m·K) Show Material materials with Conductividad térmica of 88 - 151 W/(m·K) | Typical for Rhodium |
Temperatura de fusión | 1963 °C Show Material materials with Temperatura de fusión of 1963 °C | Typical for Rhodium |