General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.19 g/cm³ Show Material materials with Densidad of 7.19 g/cm³ | Typical for Chromium |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.21 [-] Show Material materials with Coeficiente de Poisson of 0.21 [-] | Typical for Chromium |
Límite elástico | 20.0 °C | 590 MPa Show Material materials with Límite elástico of 590 MPa | |
Módulo de cizallamiento | 23.0 °C | 115 GPa Show Material materials with Módulo de cizallamiento of 115 GPa | Typical for Chromium |
Módulo elástico | 23.0 °C | 279 GPa Show Material materials with Módulo elástico of 279 GPa | Typical for Chromium |
Resistencia a la tracción | 20.0 °C | 760 MPa Show Material materials with Resistencia a la tracción of 760 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 442 - 487 J/(kg·K) Show Material materials with Calor específico of 442 - 487 J/(kg·K) | Typical for Chromium |
Coeficiente de dilatación térmica | 23.0 °C | 4.9E-6 - 8.2E-6 1/K Show Material materials with Coeficiente de dilatación térmica of 4.9E-6 - 8.2E-6 1/K | Typical for Chromium |
Conductividad térmica | 23.0 °C | 87 - 91 W/(m·K) Show Material materials with Conductividad térmica of 87 - 91 W/(m·K) | Typical for Chromium |
Temperatura de fusión | 1875 °C Show Material materials with Temperatura de fusión of 1875 °C | Typical for Chromium |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.25 % Show Material materials with Aluminio of 0.25 % |
Azufre | 0.02 % Show Material materials with Azufre of 0.02 % |
Carbono | 0.1 % Show Material materials with Carbono of 0.1 % |
Cromo | 58 - 62 % Show Material materials with Cromo of 58 - 62 % |
Fósforo | 0.02 % Show Material materials with Fósforo of 0.02 % |
Hierro | 1 % Show Material materials with Hierro of 1 % |
Manganeso | 0.3 % Show Material materials with Manganeso of 0.3 % |
Nitrógeno | 0.3 % Show Material materials with Nitrógeno of 0.3 % |
Silicona | 1 % Show Material materials with Silicona of 1 % |
Titanio | 0.5 % Show Material materials with Titanio of 0.5 % |