Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Vickers | 20.0 °C | 150 [-] Show Material materials with Dureza Vickers of 150 [-] |
Módulo elástico | 20.0 °C | 190 GPa Show Material materials with Módulo elástico of 190 GPa |
100.0 °C | 187 GPa Show Material materials with Módulo elástico of 187 GPa | |
150.0 °C | 185 GPa Show Material materials with Módulo elástico of 185 GPa | |
200.0 °C | 183 GPa Show Material materials with Módulo elástico of 183 GPa | |
230.0 °C | 182 GPa Show Material materials with Módulo elástico of 182 GPa | |
Chemical properties
Property | Value |
---|---|
Carbono | 3E-3 - 5E-3 % Show Material materials with Carbono of 3E-3 - 5E-3 % |
Hidrógeno | 5E-4 - 1E-3 % Show Material materials with Hidrógeno of 5E-4 - 1E-3 % |
Hierro | 0.01 % Show Material materials with Hierro of 0.01 % |
Molibdeno | 0.01 - 0.02 % Show Material materials with Molibdeno of 0.01 - 0.02 % |
Niobio | 0.04 - 0.1 % Show Material materials with Niobio of 0.04 - 0.1 % |
Nitrógeno | 3E-3 - 5E-3 % Show Material materials with Nitrógeno of 3E-3 - 5E-3 % |
Níquel | 5E-3 % Show Material materials with Níquel of 5E-3 % |
Silicona | 2.5E-3 - 5E-3 % Show Material materials with Silicona of 2.5E-3 - 5E-3 % |
Titanio | 4E-3 - 5E-3 % Show Material materials with Titanio of 4E-3 - 5E-3 % |
Wolframio | 2.2 - 3.5 % Show Material materials with Wolframio of 2.2 - 3.5 % |