General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 9.6 g/cm³ Show Material materials with Densidad of 9.6 g/cm³ | Typical for Lead Antimony |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell | 20.0 °C | 18 [-] Show Material materials with Dureza Brinell of 18 [-] |
50.0 °C | 15 [-] Show Material materials with Dureza Brinell of 15 [-] | |
120.0 °C | 14 [-] Show Material materials with Dureza Brinell of 14 [-] | |
150.0 °C | 10 [-] Show Material materials with Dureza Brinell of 10 [-] | |
Límite elástico Rp 0,2 | 20.0 °C | 39 MPa Show Material materials with Límite elástico Rp 0,2 of 39 MPa |
50.0 °C | 37 MPa Show Material materials with Límite elástico Rp 0,2 of 37 MPa | |
100.0 °C | 25 MPa Show Material materials with Límite elástico Rp 0,2 of 25 MPa | |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 130 - 159 J/(kg·K) Show Material materials with Calor específico of 130 - 159 J/(kg·K) | Typical for Lead Antimony |
Conductividad térmica | 23.0 °C | 24 - 34 W/(m·K) Show Material materials with Conductividad térmica of 24 - 34 W/(m·K) | Typical for Lead Antimony |
Temperatura de fusión | 235 - 305 °C Show Material materials with Temperatura de fusión of 235 - 305 °C | Typical for Lead Antimony |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.01 % Show Material materials with Aluminio of 0.01 % |
Antimonio | 13.5 - 15.5 % Show Material materials with Antimonio of 13.5 - 15.5 % |
Arsénico | 0.8 - 1.2 % Show Material materials with Arsénico of 0.8 - 1.2 % |
Bismuto | 0.1 % Show Material materials with Bismuto of 0.1 % |
Cobre | 0.7 % Show Material materials with Cobre of 0.7 % |
Estaño | 0.9 - 1.7 % Show Material materials with Estaño of 0.9 - 1.7 % |
Hierro | 0.1 % Show Material materials with Hierro of 0.1 % |
Zinc | 0.01 % Show Material materials with Zinc of 0.01 % |