Aplicaciones térmicas
Property | Value |
---|---|
Temperatura de fusión | 260 °C Show Material materials with Temperatura de fusión of 260 °C |
General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 10.3 g/cm³ Show Material materials with Densidad of 10.3 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Límite elástico Rp 0,2 | 20.0 °C | 27 - 39 MPa Show Material materials with Límite elástico Rp 0,2 of 27 - 39 MPa |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.01 % Show Material materials with Aluminio of 0.01 % |
Antimonio | 9 - 11 % Show Material materials with Antimonio of 9 - 11 % |
Arsénico | 0.25 % Show Material materials with Arsénico of 0.25 % |
Bismuto | 0.1 % Show Material materials with Bismuto of 0.1 % |
Cobre | 0.7 % Show Material materials with Cobre of 0.7 % |
Estaño | 5 - 7 % Show Material materials with Estaño of 5 - 7 % |
Hierro | 0.1 % Show Material materials with Hierro of 0.1 % |
Zinc | 0.01 % Show Material materials with Zinc of 0.01 % |