Description

Excellent formability. High strength for foil app compared to 1xxx.

Related Standards

Equivalent Materials

This material data has been provided by Aludium.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValue

Density

23.0 °C

2.72 g/cm³

Show Supplier Material materials with Density of 2.72 g/cm³

Dimension

PropertyValue

Thickness

0.06 - 1 mm

Show Supplier Material materials with Thickness of 0.06 - 1 mm

Mechanical

PropertyTemperatureValue

Elongation A50

23.0 °C

1 %

Show Supplier Material materials with Elongation A50 of 1 %

Tensile strength

23.0 °C

170 - 175 MPa

Show Supplier Material materials with Tensile strength of 170 - 175 MPa

Yield strength

23.0 °C

155 MPa

Show Supplier Material materials with Yield strength of 155 MPa

Thermal

PropertyTemperatureValue

Coefficient of thermal expansion

100.0 °C

2.4E-5 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 2.4E-5 1/K

Chemical properties

PropertyValue

Copper

0.05 %

Show Supplier Material materials with Copper of 0.05 %

Iron

0.7 - 1.3 %

Show Supplier Material materials with Iron of 0.7 - 1.3 %

Silicon

0.05 - 0.3 %

Show Supplier Material materials with Silicon of 0.05 - 0.3 %

Zinc

0.1 %

Show Supplier Material materials with Zinc of 0.1 %

Technological properties

Property
Application areas

Roofing: Foil for bituminous coating; Heat exchangers: Fins, Heat exchangers; Insulation; Semi-rigid and corrugated: Pet food; Foil stock: Foil app; Components: Automotive fins, Heat exchangers

Corrosion properties

Moderated

Workability

Excellent