General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Density | 1.2 g/cm³ Show Supplier Material materials with Density of 1.2 g/cm³ | dry | ISO 1183 |
Mechanical
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Elastic modulus | 0.14 GPa Show Supplier Material materials with Elastic modulus of 0.14 GPa | dry | ISO 527-1/-2 | |
Elongation | 350 % Show Supplier Material materials with Elongation of 350 % | dry | ISO 527-1/-2 | |
Hardness, Shore D | 45 [-] Show Supplier Material materials with Hardness, Shore D of 45 [-] | dry | ISO 868 | 3s |
Tear strength | 94 kN/m Show Supplier Material materials with Tear strength of 94 kN/m | dry | ISO 34-1; Method B | |
Tensile strength | 21 MPa Show Supplier Material materials with Tensile strength of 21 MPa | dry | ISO 527-1/-2 |
Thermal
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Heat deflection temperature | 65 °C Show Supplier Material materials with Heat deflection temperature of 65 °C | dry | ISO 75-1/-2 | 0.45 MPa | |
Melting point | 220 °C Show Supplier Material materials with Melting point of 220 °C | dry | ISO 11357-1/-3 | 10°C/min | |
Vicat softening temperature | 189 °C Show Supplier Material materials with Vicat softening temperature of 189 °C | dry | ISO 306 | 50°C/h 10N |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Melt volume-flow rate | 230 °C | 39 cm³/10min Show Supplier Material materials with Melt volume-flow rate of 39 cm³/10min | dry | ISO 1133 | |
Shrinkage | 1.6 % Show Supplier Material materials with Shrinkage of 1.6 % | dry | Sim. to ISO 294-4 | Parallel | |
1.8 % Show Supplier Material materials with Shrinkage of 1.8 % | dry | Sim. to ISO 294-4 | Normal |
Technological properties
Property | ||
---|---|---|
Application areas | Bed Springs, Railway Pads, Cosmetic Dispensers, Soap dispensers, Support Springs, Non-pneumatic wheel, Non-pneumatic wheel |