General
Property | Temperature | Value |
---|---|---|
Density | 23.0 °C | 2.66 g/cm³ Show Supplier Material materials with Density of 2.66 g/cm³ |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 70 GPa Show Supplier Material materials with Elastic modulus of 70 GPa | |
Elongation | 23.0 °C | 18 - 25 % Show Supplier Material materials with Elongation of 18 - 25 % | |
Hardness, HBW | 23.0 °C | 75 - 80 [-] Show Supplier Material materials with Hardness, HBW of 75 - 80 [-] | Test method: 2.5/62.5 |
Tensile strength | 23.0 °C | 250 - 280 MPa Show Supplier Material materials with Tensile strength of 250 - 280 MPa | |
Yield strength Rp0.2 | 23.0 °C | 115 - 130 MPa Show Supplier Material materials with Yield strength Rp0.2 of 115 - 130 MPa |
Thermal
Property | Temperature | Value |
---|---|---|
Coefficient of thermal expansion | 23.0 °C | 2.33E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 2.33E-5 1/K |
Specific heat capacity | 23.0 °C | 900 J/(kg·K) Show Supplier Material materials with Specific heat capacity of 900 J/(kg·K) |
Thermal conductivity | 23.0 °C | 110 - 130 W/(m·K) Show Supplier Material materials with Thermal conductivity of 110 - 130 W/(m·K) |
Electrical
Property | Temperature | Value |
---|---|---|
Electrical conductivity | 23.0 °C | 1.60E+7 - 1.80E+7 S/m Show Supplier Material materials with Electrical conductivity of 1.60E+7 - 1.80E+7 S/m |
Technological properties
Property | ||
---|---|---|
Other | Non heat treatable | |
Processing history | Temper: O3 |