General
Property | Temperature | Value |
---|---|---|
Density | 23.0 °C | 2.79 g/cm³ Show Supplier Material materials with Density of 2.79 g/cm³ |
Mechanical
Property | Temperature | Value |
---|---|---|
Elastic modulus | 23.0 °C | 88 GPa Show Supplier Material materials with Elastic modulus of 88 GPa |
Elongation A50 | 23.0 °C | 0.6 % Show Supplier Material materials with Elongation A50 of 0.6 % |
Hardness, Vickers, 30 | 23.0 °C | 175 [-] Show Supplier Material materials with Hardness, Vickers, 30 of 175 [-] |
Thermal
Property | Temperature | Value |
---|---|---|
Coefficient of thermal expansion | 23.0 °C | 1.79E-5 - 1.89E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 1.79E-5 - 1.89E-5 1/K |
Melting point | 518.9 °C Show Supplier Material materials with Melting point of 518.9 °C | |
Specific heat capacity | 23.0 °C | 880 J/(kg·K) Show Supplier Material materials with Specific heat capacity of 880 J/(kg·K) |
Thermal conductivity | 30.0 °C | 116.8 W/(m·K) Show Supplier Material materials with Thermal conductivity of 116.8 W/(m·K) |
Electrical
Property | Temperature | Value |
---|---|---|
Electrical conductivity | 23.0 °C | 1.28E+7 S/m Show Supplier Material materials with Electrical conductivity of 1.28E+7 S/m |
Chemical properties
Technological properties
Property | ||
---|---|---|
Application areas | Powertrain Applications, Hydraulics, Automotive | |
Processing history | Spray Compaction, Extrusion, T6 Heat Treatment |