Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 1.4 g/cm³ Show Supplier Material materials with Density of 1.4 g/cm³ | ISO 1183 |
Recycled Content | 35 % Show Supplier Material materials with Recycled Content of 35 % | ||
Water absorption | 23.0 °C | 0.06 % Show Supplier Material materials with Water absorption of 0.06 % | ASTM D570, 23°C/24hr |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Flexural modulus | 23.0 °C | 5 GPa Show Supplier Material materials with Flexural modulus of 5 GPa | ISO 178, 2 mm/min |
Flexural strength | 23.0 °C | 160 MPa Show Supplier Material materials with Flexural strength of 160 MPa | ISO 178, 2 mm/min |
Impact strength, Charpy notched | 23.0 °C | 9 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 9 kJ/m² | ISO 179eA |
Impact strength, Charpy unnotched | 23.0 °C | 40 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 40 kJ/m² | ISO 179eA |
Tensile strength | 23.0 °C | 102 MPa Show Supplier Material materials with Tensile strength of 102 MPa | ISO 527, 5 mm/min |
Thermal
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Ash content | 23.0 °C | 15 % Show Supplier Material materials with Ash content of 15 % | ASTM D5630 | ||
Heat deflection temperature, 1.80 MPa | 186 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 186 °C | ISO-75 | |||
Melting point | 240 °C Show Supplier Material materials with Melting point of 240 °C | ISO 3146 | |||
Flammability | HB for 3.2 mm sample UL94 |
Electrical
Property | Temperature | Value | Comment |
---|---|---|---|
Dielectric strength | 23.0 °C | 32 kV/mm Show Supplier Material materials with Dielectric strength of 32 kV/mm | ASTM D149, 1.6 mm, 500V/s in oil |
Dissipation factor, 1kHz | 23.0 °C | 2E-3 [-] Show Supplier Material materials with Dissipation factor, 1kHz of 2E-3 [-] | ASTM D150 |
Surface resistivity | 23.0 °C | 1.00E+15 Ω/sq Show Supplier Material materials with Surface resistivity of 1.00E+15 Ω/sq | ASTM D257 |
Volume resistivity | 23.0 °C | 8.00E+16 Ω·cm Show Supplier Material materials with Volume resistivity of 8.00E+16 Ω·cm | ASTM D257 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Shrinkage | 23.0 °C | 0.4 - 0.5 % Show Supplier Material materials with Shrinkage of 0.4 - 0.5 % | ASTM D955 |
Shrinkage, transverse | 23.0 °C | 0.5 - 0.8 % Show Supplier Material materials with Shrinkage, transverse of 0.5 - 0.8 % | ASTM D955 |
Technological properties
Property | ||
---|---|---|
Application areas | Eelcrtical components (e.g. connectros) and structural components. | |
Certifications | RoHS,RECH,ULE Environmental Claims Validation | |
Fillers | 15% Glass Fiber | |
Processing methods |