Multi-purpose, injection molding ABS providing a favorable balance of engineering properties.

This material data has been provided by Matmatch.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.04 g/cm³

Show Material materials with Density of 1.04 g/cm³

ASTM D 792

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

2.27 GPa

Show Material materials with Elastic modulus of 2.27 GPa

ASTM D 638 | 5 mm/min

Elongation

23.0 °C

24 %

Show Material materials with Elongation of 24 %

ASTM D 638 | Type I, 5 mm/min

Elongation at yield

23.0 °C

2 %

Show Material materials with Elongation at yield of 2 %

ASTM D 638 | Type I, 5 mm/min

Flexural modulus

23.0 °C

2.2 GPa

Show Material materials with Flexural modulus of 2.2 GPa

ISO 178 | 2 mm/min

Flexural yield strength

23.0 °C

70 MPa

Show Material materials with Flexural yield strength of 70 MPa

ISO 178 | 2 mm/min

Hardness, Rockwell R

23.0 °C

112 [-]

Show Material materials with Hardness, Rockwell R of 112 [-]

ASTM D 785

Impact strength, Charpy notched

-30.0 °C

9 kJ/m²

Show Material materials with Impact strength, Charpy notched of 9 kJ/m²

ISO 179/1eA

23.0 °C

26 kJ/m²

Show Material materials with Impact strength, Charpy notched of 26 kJ/m²

ISO 179/1eA

Impact strength, Izod notched

-30.0 °C

8 kJ/m²

Show Material materials with Impact strength, Izod notched of 8 kJ/m²

ISO 180/1A

23.0 °C

22 kJ/m²

Show Material materials with Impact strength, Izod notched of 22 kJ/m²

ISO 180/1A

Unlock all property charts

Impact strength, Izod notched, ASTM

23.0 °C

320 J/m

Show Material materials with Impact strength, Izod notched, ASTM of 320 J/m

ASTM D 256

Tensile strength

23.0 °C

33 MPa

Show Material materials with Tensile strength of 33 MPa

ASTM D 638 | Type I, 5 mm/min

Yield strength

23.0 °C

44 MPa

Show Material materials with Yield strength of 44 MPa

ASTM D 638 | Type I, 5 mm/min

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

8.82E-5 1/K

Show Material materials with Coefficient of thermal expansion of 8.82E-5 1/K

ASTM E 831 | -40°C to 40°C

Coefficient of thermal expansion, transverse

23.0 °C

8.82E-5 1/K

Show Material materials with Coefficient of thermal expansion, transverse of 8.82E-5 1/K

ASTM E 831 | -40°C to 40°C

Heat deflection temperature, 1.80 MPa

80 °C

Show Material materials with Heat deflection temperature, 1.80 MPa of 80 °C

ASTM D 648 | 1.82 MPa, 3.2mm, unannealed

Relative temperature index, electrical

60 °C

Show Material materials with Relative temperature index, electrical of 60 °C

UL 746B

Relative temperature index, mechanical impact

60 °C

Show Material materials with Relative temperature index, mechanical impact of 60 °C

UL 746B

Relative temperature index, mechanical strength

60 °C

Show Material materials with Relative temperature index, mechanical strength of 60 °C

UL 746B

Vicat softening temperature

99 °C

Show Material materials with Vicat softening temperature of 99 °C

ASTM D 1525 | Rate B/50

Flammability

UL Recognized, 94HB Flame Class Rating | 1.5mm | UL 94

Electrical

PropertyTemperatureValueComment

Comparative tracking index

23.0 °C

0 V

Show Material materials with Comparative tracking index of 0 V

UL 746A

Rheological Properties

PropertyTemperatureValueComment

Melt mass-flow rate

18 g/10min

Show Material materials with Melt mass-flow rate of 18 g/10min

ISO 1133 | 220°C/10.0 kg

Melt viscosity

23.0 °C

225 Pa·s

Show Material materials with Melt viscosity of 225 Pa·s

ASTM D 3825 | 240°C, 1000 sec⁻¹

Shrinkage

23.0 °C

0.5 - 0.8 %

Show Material materials with Shrinkage of 0.5 - 0.8 %

SABIC method | 3.2 mm

Technological properties

Property
Application areas

Air Cabin Interiors,Air Filtration,Amusement Machine,Animal Testing,Applique,Audio,Auto Aftermarket,Building Accessory,Building Element,Circuit Protection,Cluster,Coffee Maker/Espresso Machine,Commercial Storage/Cookware,Console,Data Management,Data Transfer,Dishwasher,Displays,Document Handling,Door Handle,Electronic Components,Enclosure/Housing/Cover,Enclosures,Energy Management,Exterior Mirror,Exterior Trim,Food Container,Food Transportation,Front Grille,Fused Deposition Modeling (FDM),Gas/Electric Oven,Head Protection,Heavy Vehicles,Industrial Material Handling,Interior,Lab Ware and Clinical Diagnostics,Laundry Dryer,Lawn/Garden,Medical Device,Medical Facility Infrastructure,Meter Water,Non-LED Lighting,Overhead,Personal Computing,Personal Water Craft,Pharmaceutical Manufacturing,Pharmaceutical Packaging & Drug Delivery,Power Manangement,Pump,Rear/Signal Lighting,Refrigerator,Respiratory,Security/Detection,Small Appliance,Storage/Table,Surgical Devices,Swimming Pool/Spa,Travel Suitcase,Vacuum Cleaner,Vending Machine,Washing Machine,Water Treatment/Filtration,Wearables,Wireless Communications,Wiring Devices

Processing methods

Drying Temperature: 80-95°C, Drying Time: 2-4hrs, Drying Time (Cumulative): 8hrs, Maximum Moisture Content: 0.1%, Melt Temperature: 220-260°C, Nozzle Temperature: 220-260°C, Front - Zone 3 Temperature: 215-240°C, Middle - Zone 2 Temperature: 205-225°C, Rear - Zone 1 Temperature: 190-210°C, Mold Temperature: 50-70°C, Back Pressure: 0.3-0.7MPa, Screw Speed: 30-60rpm, Shot to Cylinder Size: 50-70%, Vent Depth: 0.038-0.051mm