General
Property | Value |
---|---|
Density | 1.04 - 1.06 g/cm³ Show Material materials with Density of 1.04 - 1.06 g/cm³ |
Mechanical
Property | Value | Comment |
---|---|---|
Elastic modulus | 2.0 - 2.8 GPa Show Material materials with Elastic modulus of 2.0 - 2.8 GPa | |
Elongation | 10.0 - 50.0 % Show Material materials with Elongation of 10.0 - 50.0 % | |
Impact strength, Charpy notched | 2.0 - 8.0 kJ/m² Show Material materials with Impact strength, Charpy notched of 2.0 - 8.0 kJ/m² | |
Impact strength, Charpy unnotched | 30 kJ/m² Show Material materials with Impact strength, Charpy unnotched of 30 kJ/m² | |
Tensile strength | 30.0 - 38.0 MPa Show Material materials with Tensile strength of 30.0 - 38.0 MPa | at 4-7% strain |
Thermal
Property | Value |
---|---|
Coefficient of thermal expansion | 7e-05 - 0.00011 1/K Show Material materials with Coefficient of thermal expansion of 7e-05 - 0.00011 1/K |
Melting point | 160.0 - 168.0 °C Show Material materials with Melting point of 160.0 - 168.0 °C |
Specific heat capacity | 1490.0 - 1520.0 J/(kg·K) Show Material materials with Specific heat capacity of 1490.0 - 1520.0 J/(kg·K) |
Thermal conductivity | 0.41 W/(m·K) Show Material materials with Thermal conductivity of 0.41 W/(m·K) |
Flammability | UL 94 HB |
Electrical
Property | Value |
---|---|
Dielectric constant | 2.4 [-] Show Material materials with Dielectric constant of 2.4 [-] |
2.8 [-] Show Material materials with Dielectric constant of 2.8 [-] | |
Electrical resistivity | 100000000000.0 - 100000000000000.0 Ω·m Show Material materials with Electrical resistivity of 100000000000.0 - 100000000000000.0 Ω·m |
Optical
Property | Value |
---|---|
Transparency | no |
Technological properties
Property | ||
---|---|---|
Application areas | automotive interior trims, instrument panels, exterior trims, dishwasher parts | |
Fillers | 20% Talc | |
Other | You are viewing a generic polymer page, for more information please contact the suppliers or Matmatch, or use our Search under the following link to find more specific grades and formulations based on your application: Polymer Advanced Search | |
Processing methods | Injection molding, blow molding, extrusion, thermoforming |