Chromium Molybdenum Steel
ASTM A829 Grade 4142 As-Rolled, Annealed, Normalized, Normalized and Tempered, or Quenched and Tempered; Tensile strength range 100 MPaGeliefert von:
1 Matmatch-Lieferant
Chromium Molybdenum Steel
ASTM A829 Grade 4140 As-Rolled, Annealed, Normalized, Normalized and Tempered, or Quenched and Tempered; Tensile strength range 100 MPaGeliefert von:
1 Matmatch-Lieferant
Nickel Chromium Iron Alloy
DIN 17744 Grade NiCr19NbMo precipitation hardened (+P)Medium Carbon Steel
DIN 17200 Grade C40 normalized or normalized formed (+N)Silicon Steel
EN 10089 Grade 38Si7 quenched and tempered (+QT)Medium Carbon Steel
DIN 17200 Grade C40 quenched and tempered (+QT)Martensitischer Edelstahl
EN 10088-1 Grade X39Cr13 quenched and tempered (+QT800)Medium Carbon Steel
EN 10132-3 Grade C40E soft annealed or soft annealed and skin passed (+A or +A+LC)Chromium Molybdenum Steel
DIN 17240 Grade 40CrMoV4-7 quenched and tempered (+QT)Medium Carbon Steel
EN 10083-2 Grade C40 quenched and tempered (+QT)Medium Carbon Steel
EN 10277-2 Grade C40 cold drawnMedium Carbon Steel
EN 10277-5 Grade C40E quenched and tempered and cold drawn (+QT+C)