General
Property | Value | Comment |
---|---|---|
Density | 7.8 - 7.9 g/cm³ Show Material materials with Density of 7.8 - 7.9 g/cm³ | Typical for Chromium Molybdenum Steel |
Mechanical
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Elastic modulus | 200 - 215 GPa Show Material materials with Elastic modulus of 200 - 215 GPa | Typical for Chromium Molybdenum Steel | |||
Elongation | 15.0 % Show Material materials with Elongation of 15.0 % | Predicted Value, Transverse | |||
16.6 % Show Material materials with Elongation of 16.6 % | Predicted Value, A200 | ||||
18.1 % Show Material materials with Elongation of 18.1 % | Predicted Value, A80 | ||||
18.4 % Show Material materials with Elongation of 18.4 % | Predicted Value, A5 | ||||
19.0 % Show Material materials with Elongation of 19.0 % | Predicted Value, A80 Transverse | ||||
20.1 % Show Material materials with Elongation of 20.1 % | Predicted Value, A50 | ||||
20.5 % Show Material materials with Elongation of 20.5 % | Predicted Value | ||||
Hardness, Brinell | 235 [-] Show Material materials with Hardness, Brinell of 235 [-] | Predicted Value, Transverse | |||
Poisson's ratio | 0.29 [-] Show Material materials with Poisson's ratio of 0.29 [-] | Typical for Chromium Molybdenum Steel | |||
Reduction of area | 41.6 % Show Material materials with Reduction of area of 41.6 % | Predicted Value, Transverse | |||
43.2 % Show Material materials with Reduction of area of 43.2 % | Predicted Value | ||||
Shear modulus | 79.6 GPa Show Material materials with Shear modulus of 79.6 GPa | Predicted Value | |||
Shear strength | 516.9 MPa Show Material materials with Shear strength of 516.9 MPa | Predicted Value | |||
Tensile strength | 480 MPa Show Material materials with Tensile strength of 480 MPa | As-Rolled, Annealed, Normalized, Normalized and Tempered, or Quenched and Tempered; Tensile strength range 100 MPa | ASTM A829 | Plate |
Thermal
Property | Value | Comment |
---|---|---|
Coefficient of thermal expansion | 1.1e-05 - 1.4e-05 1/K Show Material materials with Coefficient of thermal expansion of 1.1e-05 - 1.4e-05 1/K | Typical for Chromium Molybdenum Steel |
Max service temperature | 256.5 °C Show Material materials with Max service temperature of 256.5 °C | Predicted Value, Long |
Melting point | 1382 - 1529 °C Show Material materials with Melting point of 1382 - 1529 °C | Typical for Chromium Molybdenum Steel |
Specific heat capacity | 448 - 502 J/(kg·K) Show Material materials with Specific heat capacity of 448 - 502 J/(kg·K) | Typical for Chromium Molybdenum Steel |
Thermal conductivity | 36 - 43 W/(m·K) Show Material materials with Thermal conductivity of 36 - 43 W/(m·K) | Typical for Chromium Molybdenum Steel |
Electrical
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Carbon | 0.38 - 0.46 % Show Material materials with Carbon of 0.38 - 0.46 % | As-Rolled, Annealed, Normalized, Normalized and Tempered, or Quenched and Tempered; Tensile strength range 100 MPa | ASTM A829 | Plate |
Chromium | 0.8 - 1.1 % Show Material materials with Chromium of 0.8 - 1.1 % | As-Rolled, Annealed, Normalized, Normalized and Tempered, or Quenched and Tempered; Tensile strength range 100 MPa | ASTM A829 | Plate |
Manganese | 0.75 - 1 % Show Material materials with Manganese of 0.75 - 1 % | As-Rolled, Annealed, Normalized, Normalized and Tempered, or Quenched and Tempered; Tensile strength range 100 MPa | ASTM A829 | Plate |
Molybdenum | 0.15 - 0.25 % Show Material materials with Molybdenum of 0.15 - 0.25 % | As-Rolled, Annealed, Normalized, Normalized and Tempered, or Quenched and Tempered; Tensile strength range 100 MPa | ASTM A829 | Plate |
Phosphorus | 0.03 % Show Material materials with Phosphorus of 0.03 % | As-Rolled, Annealed, Normalized, Normalized and Tempered, or Quenched and Tempered; Tensile strength range 100 MPa | ASTM A829 | Plate |
Silicon | 0.15 - 0.35 % Show Material materials with Silicon of 0.15 - 0.35 % | As-Rolled, Annealed, Normalized, Normalized and Tempered, or Quenched and Tempered; Tensile strength range 100 MPa | ASTM A829 | Plate |
Sulfur | 0.04 % Show Material materials with Sulfur of 0.04 % | As-Rolled, Annealed, Normalized, Normalized and Tempered, or Quenched and Tempered; Tensile strength range 100 MPa | ASTM A829 | Plate |
Technological properties
Property | ||
---|---|---|
Supplier Disclaimer | The given information is a rough description and some properties can depend on various factors such as product thickness. Please contact the supplier or refer to the related norm or standard for further information. |