Coefficient of friction: 0.18 [-]

Quick Comparison

Polyvinylidenefluoride (PVDF)

Kynar® 370

Geliefert von:

Arkema: High Performance Polymers

Polycarbonat (PC)

LNP™ LUBRICOMP™ Compound DL003

Geliefert von:

Sabic

Polyphenylene Sulfide (PPS)

LNP™ LUBRICOMP™ Compound OL004

Geliefert von:

Sabic

Polycarbonat (PC)

LNP™ LUBRILOY™ Compound D2000P

Geliefert von:

Sabic

Polyamide 66 (PA66)

LNP™ LUBRILOY™ Compound RX05497

Geliefert von:

Sabic

Polycarbonat (PC)

LNP™ LUBRICOMP™ Compound DL0039EF

Geliefert von:

Sabic

Polycarbonat (PC)

LNP™ LUBRICOMP™ Compound NXCY620

Geliefert von:

Sabic

Polyoxymethylen (POM)

LNP™ LUBRICOMP™ Compound KL003LH

Geliefert von:

Sabic

Polyamide 66 (PA66)

LNP™ LUBRICOMP™ Compound RL4040HSUV

Geliefert von:

Sabic

Polyamide 66 (PA66)

LNP™ LUBRICOMP™ Compound RP004S

Geliefert von:

Sabic

Polyoxymethylen (POM)

LNP™ LUBRICOMP™ Compound KL001

Geliefert von:

Sabic

Polyamide 610 (PA610)

LNP™ LUBRICOMP™ Compound QP004

Geliefert von:

Sabic

Polycarbonat (PC)

LNP™ LUBRICOMP™ Compound DP001E

Geliefert von:

Sabic

Polyamide 66 (PA66)

LNP™ LUBRICOMP™ Compound RP004SZ

Geliefert von:

Sabic

Polyoxymethylen (POM)

LNP™ LUBRICOMP™ Compound KX06415

Geliefert von:

Sabic

Polyoxymethylen (POM)

LNP™ LUBRICOMP™ Compound KP004L

Geliefert von:

Sabic

Polycarbonat (PC)

LNP™ LUBRILOY™ Compound D20001 - Asia

Geliefert von:

Sabic

Polyoxymethylen (POM)

LNP™ LUBRICOMP™ Compound KL004L

Geliefert von:

Sabic

Polycarbonat (PC)

LNP™ LUBRICOMP™ Compound DL002P

Geliefert von:

Sabic

Polyoxymethylen (POM)

LNP™ LUBRICOMP™ Compound KP003AXZ

Geliefert von:

Sabic
Seite 1 von 4