Kohlenstoffarmer Stahl
EN 10028-2 Grade P295GH normalized or normalized formed (+N)Geliefert von:
2 Matmatch-Lieferanten
Kohlenstoffarmer Stahl
EN 10025-2 Grade S355J0 normalized or normalized formed (+N)Geliefert von:
1 Matmatch-Lieferant
Wrought Copper High Copper Alloy
ASTM B196 Grade C17200 TB00Wrought Copper High Copper Alloy
ASTM B194 Grade C17200 TD04Wrought Copper High Copper Alloy
ASTM B768 Grade C17510 TH04Wrought Copper High Copper Alloy
EN 1652 Grade C17200 TF00Kohlenstoffarmer Stahl
EN 10273 Grade P295GH normalized or normalized formed (+N)Kohlenstoffarmer Stahl
DIN 17155 Grade 17Mn4 normalized or normalized formed (+N)Nickel Chromium Molybdenum Steel
SEW 555 Grade 23CrNiMo7-4-7 quenched and tempered (+QT)Kohlenstoffarmer Stahl
DIN 17115 Grade 15Mn3Al normalized or normalized formed (+N)Kohlenstoffarmer Stahl
DIN 17115 Grade 21Mn4Al normalized or normalized formed (+N)Nickel Chromium Steel
SEW 555 Grade 30CrMoNiV5-11 quenched and tempered (+QT)Nickel Chromium Steel
SEW 555 Grade 28CrMoNiV4-9 quenched and tempered (+QT)Nitriding Steel
EN 10085 Grade 31CrMoV9 quenched and tempered (+QT)Malleable Cast Iron
EN 1562 Grade GJMW-360-12 decarburized annealedMalleable Cast Iron
EN 1562 Grade GJMW-400-5 decarburized annealedMalleable Cast Iron
EN 1562 Grade GJMW-450-7 decarburized annealed