Materion Performance Alloys’ Alloy 3 mill hardened strip provides good strength with high electrical conductivity and good resistance to stress relaxation. It is a drop-in replacement for the obsolete Alloy 10 (C17500) strip material in Automotive, Appliance and DataCom/Telecom market applications.

Related Standards

Equivalent Materials

This material data has been provided by Materion Brush GmbH,MakeItFrom.com,Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

23.0 °C

8.75 - 8.9 g/cm³

Show Material materials with Density of 8.75 - 8.9 g/cm³

Dimension

PropertyValueComment

Diameter

1.27 - 12.7 mm

Show Material materials with Diameter of 1.27 - 12.7 mm

Length

610 - 91000 mm

Show Material materials with Length of 610 - 91000 mm

max. Rod and Bar

Outside diameter

0.76 - 76 mm

Show Material materials with Outside diameter of 0.76 - 76 mm

Rod

Thickness

0.05 - 76 mm

Show Material materials with Thickness of 0.05 - 76 mm

Bar

Width

1.27 - 559 mm

Show Material materials with Width of 1.27 - 559 mm

Wall thickness

Typically 10 to 20% of OD

Mechanical

PropertyTemperatureValueComment

Bendability 90°, bw

23.0 °C

2 [-]

Show Material materials with Bendability 90°, bw of 2 [-]

for strip with 0.25mm and thinner.

Bendability 90°, gw

23.0 °C

1 [-]

Show Material materials with Bendability 90°, gw of 1 [-]

for strip with 0.25mm and thinner.

Elastic modulus

23.0 °C

120 - 138 GPa

Show Material materials with Elastic modulus of 120 - 138 GPa

Elongation

23.0 °C

5 - 25 %

Show Material materials with Elongation of 5 - 25 %

for strip with 0.1mm and thicker.,min.

Hardness, Rockwell C

23.0 °C

18 - 26 [-]

Show Material materials with Hardness, Rockwell C of 18 - 26 [-]

Hardness, Vickers

23.0 °C

216 - 287 [-]

Show Material materials with Hardness, Vickers of 216 - 287 [-]

Shear modulus

23.0 °C

52 GPa

Show Material materials with Shear modulus of 52 GPa

Tensile strength

23.0 °C

750 - 970 MPa

Show Material materials with Tensile strength of 750 - 970 MPa

Yield strength Rp0.2

23.0 °C

650 - 900 MPa

Show Material materials with Yield strength Rp0.2 of 650 - 900 MPa

Thermal

PropertyTemperatureValue

Coefficient of thermal expansion

23.0 °C

1.6E-5 - 1.76E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.6E-5 - 1.76E-5 1/K

Melting point

1030 - 1040 °C

Show Material materials with Melting point of 1030 - 1040 °C

Specific heat capacity

23.0 °C

390 J/(kg·K)

Show Material materials with Specific heat capacity of 390 J/(kg·K)

Thermal conductivity

23.0 °C

167 - 260 W/(m·K)

Show Material materials with Thermal conductivity of 167 - 260 W/(m·K)

Electrical

PropertyTemperatureValue

Electrical resistivity

23.0 °C

3.8E-8 - 3.8E-6 Ω·m

Show Material materials with Electrical resistivity of 3.8E-8 - 3.8E-6 Ω·m

Specific Electrical conductivity

45 - 60 % IACS

Show Material materials with Specific Electrical conductivity of 45 - 60 % IACS

Chemical properties

PropertyValueComment

Aluminium

0 - 0.2 %

Show Material materials with Aluminium of 0 - 0.2 %

Beryllium

0.2 - 0.6 %

Show Material materials with Beryllium of 0.2 - 0.6 %

Cobalt

0 - 0.3 %

Show Material materials with Cobalt of 0 - 0.3 %

Copper

95.9 - 98.4 %

Show Material materials with Copper of 95.9 - 98.4 %

Balance

Iron

0 - 0.1 %

Show Material materials with Iron of 0 - 0.1 %

Nickel

1.4 - 2.2 %

Show Material materials with Nickel of 1.4 - 2.2 %

Other

0 - 0.5 %

Show Material materials with Other of 0 - 0.5 %

Silicon

0 - 0.2 %

Show Material materials with Silicon of 0 - 0.2 %

Technological properties

Property
Application areas

Typical applications include high reliability spring contacts for switches and relays.,Aerospace: Landing gear, bearing bushes and high performance fasteners;Automotive: Valve guides, bushes and valve seats;Offshore & marine: Offshore drilling and instrumentation equipment, downhole tooling, valve, pump and shaft components;Other: Deep drawing tooling, plastic moulding dies, tools and plungers, die-casting plunger tips, non-magnetic and non sparking tools, electrical and electronic connectors, springs, fasteners, switchgear, resistance welding electrodes and equipment, flash butt welding dies and inserts, seam welding electrode shafts,Typical applications include resistance welding components, and inserts for metal die casting, injection molding and blow molding.,Typical applications include dies casting plunger tips and dies for steel extrusion.,Typical applications include heat exchanger tubing and resistance welding components.,Typical applications include coil springs and formed wire contacts.

Corrosion properties

High corrosion resistance

General machinability

Very good machinability