EN 1652 Grade C17200 TF00

Alternative and trade names
Alloy 190,Alloy 25 (C17200) Tube,Alloy 25 (C17200) Wire,Alloy 25 (C17200) Strip
Want to keep this datasheet? Save it now in your required format

Description

Materion Performance Alloys, Alloy 290 strip provides the highest strength of any mill hardened copper alloy, with electrical conductivity considerably greater than other high strength copper alloys. This alloy features good stress relaxation resistance and high fatigue strength.

Related Standards

Equivalent Materials

This material data has been provided by MakeItFrom.com,Materion Brush GmbH.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

23.0 °C

8.3 - 8.8 g/cm³

Show Material materials with Density of 8.3 - 8.8 g/cm³

Dimension

PropertyValue

Diameter

1.27 - 12.7 mm

Show Material materials with Diameter of 1.27 - 12.7 mm

Outside diameter

19.1 - 406 mm

Show Material materials with Outside diameter of 19.1 - 406 mm

Thickness

0.05 - 4.77 mm

Show Material materials with Thickness of 0.05 - 4.77 mm

Width

1.27 - 406.5 mm

Show Material materials with Width of 1.27 - 406.5 mm

Wall thickness

10-20% of outside diameter

Mechanical

PropertyTemperatureValueComment

Bendability 90°, bw

23.0 °C

2 - 10 [-]

Show Material materials with Bendability 90°, bw of 2 - 10 [-]

for strip with 0.25mm and thinner.

Bendability 90°, gw

23.0 °C

2 - 5 [-]

Show Material materials with Bendability 90°, gw of 2 - 5 [-]

for strip with 0.25mm and thinner.

Elastic modulus

23.0 °C

130 - 131 GPa

Show Material materials with Elastic modulus of 130 - 131 GPa

Elongation

23.0 °C

1 - 75 %

Show Material materials with Elongation of 1 - 75 %

min., for strip thicker than 0.10 mm,min.,min., for wire with 0.1mm diameter and more.

Hardness, Vickers

23.0 °C

285 - 435 [-]

Show Material materials with Hardness, Vickers of 285 - 435 [-]

Tensile strength

23.0 °C

410 - 1490 MPa

Show Material materials with Tensile strength of 410 - 1490 MPa

min.

Yield strength

23.0 °C

1110 MPa

Show Material materials with Yield strength of 1110 MPa

Yield strength Rp0.2

23.0 °C

130 - 1350 MPa

Show Material materials with Yield strength Rp0.2 of 130 - 1350 MPa

min.

Thermal

PropertyTemperatureValue

Coefficient of thermal expansion

23.0 °C

1.75E-5 - 1.8E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.75E-5 - 1.8E-5 1/K

Melting point

870 °C

Show Material materials with Melting point of 870 °C

Specific heat capacity

23.0 °C

360 J/(kg·K)

Show Material materials with Specific heat capacity of 360 J/(kg·K)

Thermal conductivity

23.0 °C

105 - 110 W/(m·K)

Show Material materials with Thermal conductivity of 105 - 110 W/(m·K)

Electrical

PropertyTemperatureValue

Electrical resistivity

23.0 °C

6.2E-8 - 7.8E-6 Ω·m

Show Material materials with Electrical resistivity of 6.2E-8 - 7.8E-6 Ω·m

Specific Electrical conductivity

17 - 30 % IACS

Show Material materials with Specific Electrical conductivity of 17 - 30 % IACS

Magnetic

PropertyTemperatureValueComment

Relative magnetic permeability

23.0 °C

1 [-]

Show Material materials with Relative magnetic permeability of 1 [-]

max.

Chemical properties

PropertyValueComment

Aluminium

0 - 0.2 %

Show Material materials with Aluminium of 0 - 0.2 %

Beryllium

1.8 - 2.2 %

Show Material materials with Beryllium of 1.8 - 2.2 %

Cobalt

0.2 %

Show Material materials with Cobalt of 0.2 %

min. Nickel + Cobalt

Copper

96.1 - 98 %

Show Material materials with Copper of 96.1 - 98 %

Balance

Iron

0 - 0.6 %

Show Material materials with Iron of 0 - 0.6 %

max., Nickel + Cobalt + Iron,max. Nickel + Cobalt + Iron

Lead

0.2 - 0.6 %

Show Material materials with Lead of 0.2 - 0.6 %

Nickel

0.2 - 0.6 %

Show Material materials with Nickel of 0.2 - 0.6 %

min. Nickel + Cobalt

Other

0 - 0.5 %

Show Material materials with Other of 0 - 0.5 %

Silicon

0 - 0.2 %

Show Material materials with Silicon of 0 - 0.2 %

Technological properties

Property
Application areas

Typical applications include high reliability spring contacts for switches and relays, battery contacts, and automotive terminals.,Typical applications include bushings and bearings for aircraft as well as drill collars and instrument housings for oil and gas exploration.,Typical applications include precision coil springs and pins for burn-in and test socket contacts and probe pins, computer processor socket contacts, cold headed fasteners, modular jack contacts, woven mesh electromagnetic shielding gaskets and resilient eyeglass frames.,Typical applications include pressure sensor bellows, burn-in and test socket contacts, computer processor socket contacts, and electromagnetic shielding gaskets.,EtchMet alloy is a material that is tailor made for the springs in voice coil motors and optical image stabilization systems common in smart phone cameras.