Wrought Copper Brass Yellow Brass
EN 1652 Grade CuZn10 O60Wrought Copper Brass Yellow Brass
EN 1652 Grade CuZn30 O60Wrought Copper Brass Yellow Brass
EN 12166 Grade CuZn36 O60Wrought Copper Pure / Low Alloyed Copper
EN 12163 Grade Cu-DLP O60Wrought Copper Brass Yellow Brass
EN 12166 Grade CuZn15 O60Wrought Copper Bronze Silicon Bronze
EN 1652 Grade CuNi2Si TB00Phosphorbronze
EN 12163 Grade CuSn6 R340Wrought Copper Brass Yellow Brass
EN 1652 Grade CuZn37 O60